Open Research Data - Electrochemical properties of porous Sr0.86Ti0.65Fe0.35O3 oxygen electrodes
Filters
total: 15
Open Research Data Series
-
X-ray diffractometry results of the Sr0.86Ti0.65Fe0.35O3 powder
Open Research DataThis dataset contains results of X-ray diffractometry mesurement (XRD) of the Sr0.86Ti0.65Fe0.35O3-d (STF35) powder. The phase composition of the investigated STF35 powder was analyzed by XRD at room temperature. It confirms the formation of the cubic perovskite oxide phase. Calculated average lattice constant is a 3.90882(1) Å, with Goodness of Fit...
-
Electrical conductivity of the Sr0.86Ti0.65Fe0.35O3-d pellet at different oxygen partial pressures
Open Research DataThis dataset contains results electrical conductivity measurements of dense Sr0.86Ti0.65Fe0.35O3-d (STF35) pellet. DC electrical conductivity measurements of STF35 were performed by the Van der Pauw method. Studies were performed at different oxygen partial pressures (20%, 1% and 0.1%) under humidified (~4 vol%) gas flow rate of 50 ml min -1.
-
Series resistance (at 800 °C - 500 °C) of the Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes sintered at different temperatures
Open Research DataIn this dataset are presented results of the ohmic contribution of differently sintered Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C, 1000 °C and 1050 °C. The measurement temperature range was between 800 °C and 500 °C in stationary air. Results converted to electrode surfaces area.
-
Area specific resistance (at 800 °C - 500 °C) of the Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes sintered at different temperatures
Open Research DataIn this dataset are presented results of the polarization resistance of differently sintered Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C, 1000 °C and 1050 °C. The measurement temperature range was between 800 °C and 500 °C in stationary air. Results converted to electrode surfaces...
-
SEM images of cross sections of porous Sr0.86Ti0.65Fe0.35O3 oxygen electrodes sintered at different temperatures
Open Research DataThis dataset contains cross sectional images of the porous Sr0.86Ti0.65Fe0.35O3 oxygen electrodes symmetric cells samples interface. Here are presented images of electrodes sintered at 950 °C, 1000 °C and 1050 °C. Images were obtained using a FEI Quanta FEG 250 Scanning Electron Microscope (SEM) with an accelerating voltage of 10 kV in a high vacuum...
-
Distribution of Relaxation Times analysis results of impedance of porous Sr0.86Ti0.65Fe0.35O3 oxygen electrode (sintered at 1000 °C) as a function of oxygen partial pressure at 800 °C
Open Research DataThis dataset contains results of Distribution of Relaxation Times analysis (DRT) of impedance of porous Sr0.86Ti0.65Fe0.35O3 oxygen electrode as a function of oxygen partial pressure at 800 °C. Electrode was sintered at 1000 °C and measured at different oxygen partial pressures (10% pO2, 1% pO2, 0.1% pO2).
-
Distribution of Relaxation Times analysis results of impedance of porous Sr0.86Ti0.65Fe0.35O3 oxygen electrode (sintered at 1000 °C) as a function of measuring temperature at 0.1% pO2
Open Research DataThis dataset contains results of Distribution of Relaxation Times analysis (DRT) of impedance of porous Sr0.86Ti0.65Fe0.35O3 oxygen electrode as a function of measuring temperature at 0.1% pO2. Electrode was sintered at 1000 °C and measured at different temperatures (800 °C, 750 °C, 700 °C).
-
Fitted impedance spectra of a symmetrical porous Sr0.86Ti0.65Fe0.35O3 oxygen electrode (sintered at 1000 °C, measured at 800 °C and 0.1% pO2) with an individual contributions of the respective fitting elements
Open Research DataThis dataset contains exemplary impedance spectra (measured at 800 °C and 0.1% pO2) for porous Sr0.86Ti0.65Fe0.35O3 oxygen electrode sintered at 1000 °C. Results of symmetric cell impedance measurement were converted to electrode surfaces area and dived by two electrodes. Dataset conatins also fitting results and individual contributions of the respective...
-
Fitted impedance spectra of a symmetrical porous Sr0.86Ti0.65Fe0.35O3 oxygen electrode (sintered at 1000 °C, measured at 700 °C and 0.1% pO2) with an individual contributions of the respective fitting elements
Open Research DataThis dataset contains exemplary impedance spectra (measured at 700 °C and 0.1% pO2) for porous Sr0.86Ti0.65Fe0.35O3 oxygen electrode sintered at 1000 °C. Results of symmetric cell impedance measurement were converted to electrode surfaces area and dived by two electrodes. Dataset conatins also fitting results and individual contributions of the respective...
-
Oxygen partial pressure and temperature dependence of series resistance of symmetrical porous Sr0.86Ti0.65Fe0.35O3 electrode on CGO substrate
Open Research DataThis dataset contains values of series resistance (R) at different temperatures (800 °C, 750 °C, 700 °C, 650 °C and 600 °C) and oxygen partial pressures (20%, 10%, 5%, 1%, 0.1% and 0.01% pO2) of symmetrical Sr0.86Ti0.65Fe0.35O3 electrode sintered at 1000 °C. This values were obtained by fitting each measured impedance spectra by electrical equivalent...
-
Oxygen partial pressure and temperature dependence of Gerischer element of symmetrical porous Sr0.86Ti0.65Fe0.35O3 electrode on CGO substrate
Open Research DataThis dataset contains values of Gericher element at different temperatures (800 °C, 750 °C, 700 °C, 650 °C and 600 °C)and oxygen partial pressures (20%, 10%, 5%, 1%, 0.1% and 0.01% pO2) of symmetrical Sr0.86Ti0.65Fe0.35O3 electrode sintered at 1000 °C. This values were obtained by fitting each measured impedance spectra by electrical equivalent circuit...
-
Oxygen partial pressure and temperature dependence of middle frequency resistance of symmetrical porous Sr0.86Ti0.65Fe0.35O3 electrode on CGO substrate
Open Research DataThis dataset contains values of middle frequency resistance at different temperatures (800 °C, 750 °C, 700 °C, 650 °C and 600 °C) and oxygen partial pressures (20%, 10%, 5%, 1%, 0.1% and 0.01% pO2) of symmetrical Sr0.86Ti0.65Fe0.35O3 electrode sintered at 1000 °C. This values were obtained by fitting each measured impedance spectra by electrical equivalent...
-
Oxygen partial pressure and temperature dependence of low frequency resistance of symmetrical porous Sr0.86Ti0.65Fe0.35O3 electrode on CGO substrate
Open Research DataThis dataset contains values of low frequency resistance at different temperatures (800 °C, 750 °C, 700 °C, 650 °C and 600 °C) and oxygen partial pressures (20%, 10%, 5%, 1%, 0.1% and 0.01% pO2) of symmetrical Sr0.86Ti0.65Fe0.35O3 electrode sintered at 1000 °C. This values were obtained by fitting each measured impedance spectra by electrical equivalent...
-
Oxygen partial pressure and temperature dependence of low frequency capacitance of symmetrical porous Sr0.86Ti0.65Fe0.35O3 electrode on CGO substrate
Open Research DataThis dataset contains values of low frequency capacitance at different temperatures (800 °C, 750 °C, 700 °C, 650 °C and 600 °C) and oxygen partial pressures (20%, 10%, 5%, 1%, 0.1% and 0.01% pO2) of symmetrical Sr0.86Ti0.65Fe0.35O3 electrode sintered at 1000 °C. This values were obtained by fitting each measured impedance spectra by electrical equivalent...
-
Oxygen partial pressure and temperature dependence of middle frequency capacitance of symmetrical porous Sr0.86Ti0.65Fe0.35O3 electrode on CGO substrate
Open Research DataThis dataset contains values of middle frequency capacitance at different temperatures (800 °C, 750 °C, 700 °C, 650 °C and 600 °C) and oxygen partial pressures (20%, 10%, 5%, 1%, 0.1% and 0.01% pO2) of symmetrical Sr0.86Ti0.65Fe0.35O3 electrode sintered at 1000 °C. This values were obtained by fitting each measured impedance spectra by electrical equivalent...