The XRD diffraction patterns of La0.3Sr1.7Al0.1Fe1.5Mo0.5O6 powder calcined at 1100oC in air - Open Research Data - Bridge of Knowledge

Search

The XRD diffraction patterns of La0.3Sr1.7Al0.1Fe1.5Mo0.5O6 powder calcined at 1100oC in air

Description

The dataset includes XRD patterns of La0.3Sr1.7Al0.1Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.

Dataset file

SLFAM_1100.raw
33.7 kB, S3 ETag 6634bb3ad58659f250b0199c76d6cc08-1, downloads: 4
The file hash is calculated from the formula
hexmd5(md5(part1)+md5(part2)+...)-{parts_count} where a single part of the file is 512 MB in size.

Example script for calculation:
https://github.com/antespi/s3md5

File details

License:
Creative Commons: by-nc 4.0 open in new tab
CC BY-NC
Non-commercial
Raw data:
Data contained in dataset was not processed.
Software:
XRD software (e.g. HighScore)

Details

Year of publication:
2021
Verification date:
2021-06-17
Creation date:
2021
Dataset language:
English
Fields of science:
  • materials engineering (Engineering and Technology)
DOI:
DOI ID 10.34808/mncs-d525 open in new tab
Verified by:
Gdańsk University of Technology

Keywords

Cite as

seen 32 times