Fractographic-fractal dimension correlation with crack initiation and fatigue life for notched aluminium alloys under bending load
Abstract
In this study, fatigue fracture surfaces of aluminium alloy 2017-T4 notched specimens were investigated under cyclic bending to find an alternative failure loading index.. The surface topographies were measured on the entire fracture area with an optical profilometer for different loading conditions. Fatigue crack initiation life Ni and total fatigue life Nf were examined using standard surface topography parameters (such as, root mean square height Sq, arithmetical mean height Sa, maximum height Sz) and non-standard surface topography parameters (such as, fractal dimension Df). Fatigue life assessment was successfully performed by combining both fracture surface topography and stress state features. The results show that the fracture plane geometry, expressed by the fractographic-fractal dimension, can facilitate the estimation of post-failure loading history.
Citations
-
2 1
CrossRef
-
0
Web of Science
-
2 2
Scopus
Authors (6)
Cite as
Full text
- Publication version
- Accepted or Published Version
- DOI:
- Digital Object Identifier (open in new tab) 10.1016/j.engfailanal.2023.107285
- License
-
open in new tab
Keywords
Details
- Category:
- Articles
- Type:
- artykuły w czasopismach
- Published in:
-
ENGINEERING FAILURE ANALYSIS
no. 149,
ISSN: 1350-6307 - Language:
- English
- Publication year:
- 2023
- Bibliographic description:
- Macek W., Rozumek D., Faszynka S., Branco R., Zhu S., Masoudi Nejad R.: Fractographic-fractal dimension correlation with crack initiation and fatigue life for notched aluminium alloys under bending load// ENGINEERING FAILURE ANALYSIS -Vol. 149, (2023), s.107285-
- DOI:
- Digital Object Identifier (open in new tab) 10.1016/j.engfailanal.2023.107285
- Sources of funding:
-
- Free publication
- Verified by:
- Gdańsk University of Technology
seen 112 times
Recommended for you
Fractal dimension for bending–torsion fatigue fracture characterisation
- W. Macek,
- R. Branco,
- M. Korpyś
- + 1 authors