Brunauer-Emmett-Teller (BET) surface analysis of titanium dioxide (TiO2) and silicon dioxide (SiO2) used for coating of expanded polystyrene spheres (EPS) - Open Research Data - Bridge of Knowledge

Search

Brunauer-Emmett-Teller (BET) surface analysis of titanium dioxide (TiO2) and silicon dioxide (SiO2) used for coating of expanded polystyrene spheres (EPS)

Description

Data refer to the results of BET surface area of TiO2 and SiO2 powders used for coating of expanded polystyrene spheres. The detailed measurement and equipment data was described in readme BET.txt file.
TiO2 was treated firstly in autoclave at 150 C degrees for 1h, then was further heat treated in Ar at 400 C degrees. As a raw material TiO2 was used, which was a semiproduct from the industrial production of titania white by sulphur method. The raw material was mostly amorphous and contained some nuclei of rutile and sulphur species. SiO2 was obtained via modified Strober method.

Dataset file

BET.zip
32.7 kB, S3 ETag db97efc2a4ce26c087c38635a0669243-1, downloads: 62
The file hash is calculated from the formula
hexmd5(md5(part1)+md5(part2)+...)-{parts_count} where a single part of the file is 512 MB in size.

Example script for calculation:
https://github.com/antespi/s3md5
download file BET.zip

File details

License:
Creative Commons: by 4.0 open in new tab
CC BY
Attribution

Details

Year of publication:
2024
Related location:
Szczecin, województwo zachodniopomorskie, Polska (53° 25′ 29″ N, 14° 32′ 8″ E)
Verification date:
2024-02-12
Creation date:
2023
Dataset language:
English
Fields of science:
  • materials engineering (Engineering and Technology)
DOI:
DOI ID 10.34808/7k25-jw97 open in new tab
Funding:
Verified by:
West Pomeranian University of Technology in Szczecin

Keywords

References

Cite as

Authors

seen 159 times