Description
This dataset contains results of dilatometry measurements of SrTi0.65Fe0.35O3-d powder. The investigation of the linear thermal expansion was carried out using a Netzsch DIL402 dilatometer. The SrTi0.65Fe0.35O3-d powder was formed into cylinders and heat up to 1100 °C with a heating rate of 5 °C min−1, dwelled for 15 min, and then cooled at a rate of 3 °C min−1. The procedure was carried out in 21% O2.
Dataset file
ExpDat_STF35 600rpm_600_air.txt
22.0 kB,
S3 ETag
bb71b077f2b15268b36e7ae7e7bcf313-1,
downloads: 55
The file hash is calculated from the formula
Example script for calculation:
https://github.com/antespi/s3md5
hexmd5(md5(part1)+md5(part2)+...)-{parts_count}
where a single part of the file is 512 MB in size.Example script for calculation:
https://github.com/antespi/s3md5
File details
- License:
-
open in new tabCC BY-NC-SANon-commercial - Share-alike
- Raw data:
- Data contained in dataset was not processed.
Details
- Year of publication:
- 2021
- Verification date:
- 2021-06-16
- Creation date:
- 2019
- Dataset language:
- English
- Fields of science:
-
- Automation, electronic and electrical engineering (Engineering and Technology)
- materials engineering (Engineering and Technology)
- DOI:
- DOI ID 10.34808/w2kz-q525 open in new tab
- Funding:
- Series:
- Verified by:
- Gdańsk University of Technology
Keywords
References
- publication Effect of sintering temperature on electrochemical performance of porous SrTi1-xFexO3-δ (x = 0.35, 0.5, 0.7) oxygen electrodes for solid oxide cells
- publication The Influence of Iron Doping on Performance of SrTi1-XFexO3-δ Perovskite Oxygen Electrode for SOFC
Cite as
Authors
seen 114 times