Description
The dataset includes the XRD pattern of CeO2/10wt.%Ni. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
Dataset file
CeO2_Ni10_no_Bc.raw
33.7 kB,
S3 ETag
62b76dba62318ccc18c151d09198075a-1,
downloads: 42
The file hash is calculated from the formula
Example script for calculation:
https://github.com/antespi/s3md5
hexmd5(md5(part1)+md5(part2)+...)-{parts_count}
where a single part of the file is 512 MB in size.Example script for calculation:
https://github.com/antespi/s3md5
File details
- License:
-
open in new tabCC BY-NCNon-commercial
- Raw data:
- Data contained in dataset was not processed.
- Software:
- XRD software (e.g. HighScore)
Details
- Year of publication:
- 2021
- Verification date:
- 2021-06-18
- Creation date:
- 2020
- Dataset language:
- English
- Fields of science:
-
- materials engineering (Engineering and Technology)
- DOI:
- DOI ID 10.34808/330a-ec69 open in new tab
- Funding:
- Verified by:
- Gdańsk University of Technology
Keywords
Cite as
Authors
seen 93 times