Abstract

In the paper has been discussed influence of stresses on general corrosion rate and corrosion pit nucleation and growth rate, whose presence has been questioned by some authors but accepted by most of them. Influence of pit walls roughness on fatigue life of a plate suffering pit corrosion and presence of so called "non damaging" pits which never lead to initiation of fatigue crack, has been presented. Possibility of prediction of pit-to-crack transition moment by two different ways, i.e. considering pit as a stress concentrator or as an equivalent crack, has been analyzed. Also, influence of statisyical distribution of corrosion pits depth as well as anticorrosion protection on fatigue and corrosion fatigue of pitted elements, have been described.

Cite as

Full text

download paper
downloaded 22 times
Publication version
Accepted or Published Version
License
Creative Commons: CC-BY-NC-ND open in new tab

Keywords

Details

Category:
Articles
Type:
artykuł w czasopiśmie wyróżnionym w JCR
Published in:
Polish Maritime Research no. 22, pages 57 - 66,
ISSN: 1233-2585
Language:
Polish
Publication year:
2015
Bibliographic description:
Jakubowski M.: Influence of pitting corrosion on fatigue and corrosion fatigue of ship and offshore structures. Part II: Load - pit crack interaction// Polish Maritime Research. -Vol. 22, iss. 3 (2015), s.57-66
Verified by:
Gdańsk University of Technology

seen 151 times

Recommended for you

Meta Tags