displaying 1000 best results Help
Search results for: 304l stainless steel
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 039_h_5
Open Research DataData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 019_h_4
Open Research DataData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 039_v_2
Open Research DataData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
3D printed ABS thermoplastic vs. steel. Dry sliding wear test in constant load & velocity ring on flat configuration. Test parameters: print layer thickness and orientation. Test symbol: 039_h_3
Open Research DataData gathered in sliding ring-on-block (flat contact) tribological experiment. Materials: alloy steel (heat treated) vs. ABS plastic.
-
Degradacja stali 9CR-1Mo pod wpływem podwyższonej temperatury. Degradation of 9Cr-1Mo steel under the influence of elevated temperature
PublicationBadano charakterystyczne cechy degradacji mikrostruktury i właściwości mechanicznych stali 9Cr-1Mo gat. P9 ASTM SA-335 po eksploatacji w piecu rafineryjnym w temperaturze 390-500 stopni C. Wykazano, że po 30 000 godzin wydłużenie obniżyło się o około 30%. Przyczyną spadku wydłużenia były zmiany mikrostruktury związane z umocnieniem osnowy metalicznej przez chrom oraz wynikające z kruchości odpuszczania stali. Większy spadek wydłużenia...
-
Experimental Study on Steel Tank Model Using Shaking Table/ Badania Eksperymentalne Modelu Zbiornika Stalowego Na Stole Sejsmicznym
PublicationStalowe zbiorniki walcowe są bardzo popularnymi konstrukcjami używanymi do magazynowania produktów przemysłu chemicznego i naftowego. Ich bezpieczeństwo i niezawodność są kluczowe, ponieważ każde uszkodzenie może nieść za sobą bardzo poważne konsekwencje. Trzęsienia ziemi są najbardziej niebezpiecznymi, a zarazem najbardziej nieprzewidywalnymi obciążeniami dynamicznymi, które mogą oddziaływać na tego typu konstrukcje. Z drugiej...
-
High-Performance Face Milling of 42CrMo4 Steel: Influence of Entering Angle on the Measured Surface Roughness, Cutting Force and Vibration Amplitude
Publication -
Abrasive Wear, Scuffing and Rolling Contact Fatigue of DLC-Coated 18CrNiMo7-6 Steel Lubricated by a Pure and Contaminated Gear Oil
Publication -
Effects of extreme pressure and anti-wear additives on surface topography and tool wear during MQCL turning of AISI 1045 steel
Publication -
Assesment of (Mn,Co)3O4powders for possible coating material for SOFC/SOEC interconnects
PublicationIn this work (Mn,Co)3O4 spinel powders with different Mn:Co ratio (1:1 and 1:2) and from different commercial suppliers are evaluated for possible powder for production of interconnect coatings. Sinterability of the powders is evaluated on pressed pellets sintered in oxidizing and in reducing/oxidizing atmospheres. For selected powder, coatings are then prepared by the electrophoretic deposition method on Crofer 22 APU stainless...
-
Fe-modified Mn2CuO4 spinel oxides: coatings based on abundant elements for solid oxide cell interconnects
PublicationThe current state of the art steel interconnect coating materials are based on critical raw material - Co-oxide spinels. Replacing Co-oxide spinels with alternative, abundant materials can reduce the dependence on the critical raw materials. Cobalt-free coatings with the general formula Mn2-xCuFexO4, where x = 0, 0.1, 0.3, were electrophoretically deposited on a ferritic stainless-steel support and evaluated. Prior to deposition,...
-
Multilayer coatings based on cerium oxide and manganese cobaltite spinel for Crofer22APU SOC interconnects
PublicationThe current state of the art steel interconnect coating materials are based on critical raw material - Co-oxide spinels. Replacing Co-oxide spinels with alternative, abundant materials can reduce the dependence on the critical raw materials. Cobalt-free coatings with the general formula Mn2-xCuFexO4, where x = 0, 0.1, 0.3, were electrophoretically deposited on a ferritic stainless-steel support and evaluated. Prior to deposition,...
-
Seismic damage diagnosis in adjacent steel and RC MRFs considering pounding effects through improved wavelet-based damage-sensitive feature
Publication -
Wpływ mikrostruktury stali o podwyższonej wytrzymałości na niszczenie wodorowe = Influence o higher strength steel microstructure on hydrogen destruction
PublicationW artykule przedstawiono niszczenie wodorowe stali 18G2A i jej symulowanej strefy wpływu ciepła (SWC). Jako parametry niszczenia wodorowego wybrano względne wartości energii zniszczenia, wydłużenia, przewężenia i wytrzymałości na rozciąganie. Parametry te wyznaczono w próbie odkształcania z małą prędkością na próbkach okrągłych gładkich. Stwierdzono, że stal 18G2A w środowisku kwaśnym podczas polaryzacji katodowej jest bardziej...
-
Atomic force microscopy based approach to local impedance measurements of grain interiors and grain boundaries of sensitized AISI 304 stanless steel
PublicationPraca prezentuje wyniki badań uzyskane z pomiarów techniką lokalnej spektroskopii impedancyjnej (LIS) wykonanych w trybie kontaktowym mikroskopii sił atomowych (AFM), które zostały przeprowadzone w lokalnych obszarach powierzchni ziarna austenitu i na granicy ziarna austenitu wysokostopowej stali austenitycznej AISI 304 poddanej procesowi uczulania oraz na próbkach odniesienia nie poddanych obróbce cieplnej.Badania LIS-AFM były...
-
The Influence of the Application of EP Additive in the Minimum Quantity Cooling Lubrication Method on the Tool Wear and Surface Roughness in the Process of Turning 316L Steel
Publication -
Experimental investigation on welding of 2.25 Cr-1.0 Mo steel with regulated metal deposition and GMAW technique incorporating metal-cored wires
Publication -
INFLUENCE OF SURFACE CURVATURE ON SESSILE DROPLET CONTACT ANGLE OF NANOFLUIDS
PublicationThis paper deals with change in contact angle of droplets of three nanofluids, i.e. water-Al2O3, water-TiO2 and water-Cu. Nanoparticles were tested at the concentration of 0.01%, 0.1%, and 1% by weight. Although dispersants were not used to stabilize the suspension, the solutions tested exhibited satisfactory stability. Ultrasonic vibration was used in order to stabilise the dispersion of the nanoparticles. Experimental measurements...
-
Electrical and mechanical characterization of two-phase alloys by means of scanning probe microscopy in dynamic impedance spectroscopy mode
PublicationDynamic impedance spectroscopy, evaluated for measuring non-stationary systems, was used in combination with scanning probe microscope. Using this approach, localized impedance measurements in the AFM contact mode could be carried out. Additionally, impedance–force curves were made at each phase of investigated materials to illustrate the relation between impedance and the force applied to a probe. Therefore, correlation of electrical...
-
3D Printing of Metallic Implants
PublicationThe fabrication of various elements, solid and open porous structures of stainless steel and Ti alloy is described. The process was started with the design of 3D models in CAD/CAM system. The 3D models were transformed into *.stl files and then the manufacturing process of the real structures by means of the selective laser melting with the SLM Realizer 100 3D printer was made. The paper shows the porous specimens made for possible...
-
Experimental investigation of forced convection of water/EGAl2O3 nanofluids inside horizontal tube
PublicationIn this paper, forced convection of water/EG-Al2O3 nanofluids inside horizontal stainless steel tube is studied experimentally. As base fluid served water/EG mixture of two ratios (60:50 and 50:50). Nanoparticle mass concentrations was 0.1% or and 1%. Transition and turbulent flow regimes were tested. Average heat transfer coefficient and pressure drop values were determined for nanofluids and compared to base fluids. Deterioration...
-
Stability and load bearing capacity of a braced truss under upward wind loading
PublicationThe paper is focused on the numerical and experimental investigation of stability of a steel truss under upward wind loading. The structure was stiffened by elastic braces situated at the top and bottom chord. Usually the lateral (translational) brace stiffness is considered. However, the rotational stiffness of braces caused by interaction between torsional stiffness of the truss top chord and bending stiffness of the roof elements...
-
The AFM topographic measurements of the surface heterogeneity of iron hexacyanoferrate on a steel surface
Open Research DataMeasurements in semi-contact mode. NTEGRA Prima (NT-MDT) device. NSG 01 probe.
-
EH36 steel for shipbuilding - Charpy impact test reslut in vary tempetatures
Open Research DataThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
The home-made in situ passive flux sampler for the measurement of monoterpene emission flux: preliminary studies
PublicationThe paper presents the construction and metrological characteristics of the home-made in situ passive flux sampler, an analytical tool representing small-scale emission chambers working in situ and passively sampling analytes from the gaseous phase. The sorption element was a cylindrical container made of stainless steel net, packed with a carbon sorbent bed-graphitized charcoal, Carbograph 4 (35/50mesh). The recommended working/exposure...
-
Karol Niklas dr hab. inż.
PeopleKarol NIKLAS is a university professor at Gdansk University of Technology (Faculty of Mechanical Engineering and Ship Technology, Institute of Naval Architecture). He defended his master's thesis on Naval Architecture, specialty Design of vessels and yachts in 2007. In 2008, he completed postgraduate studies in the specialty 'Novel Simulation Methods in Engineering' at the Faculty of Applied Physics and Mathematics. In 2014 awarded...
-
Direct measurements, numerical predictions and simple formula estimations of welding-induced biaxial residual stresses in a full-scale steel stiffened plate structure
Publication -
Analysis of Cutting Force and Power Under the Conditions of Minimized Cooling in the Process of Turning AISI-1045 Steel with the Use of the Parameter Space Investigation Method
Publication -
Surface Texture after Turning for Various Workpiece Rigidities
PublicationIn the paper, we present an analysis of the surface texture of turned parts with L/D (length/diameter) ratios of 6 and 12 and various rigidity values. The studies were carried out on samples made of S355JR steel and AISI 304 stainless steel. A detailed analysis of 2D surface profiles was carried out by using a large number of parameters that allowed us to distinguish significant differences in the surface microgeometry, which confirmed...
-
Application of galvanodynamic impedance spectroscopy for studying passive film cracking under mechanical strain
PublicationThe paper reports the results of simultaneous mechanical and electrochemical investigations on austenitic (18/8) stainless steel in a 2 % solution of sulphuric acid. The measurements were performed using Galvanodynamic Electrochemical Impedance Spectroscopy (GDEIS). Electrochemical analysis of mechanical passive layer cracking and repassivation conditions during a tensile test was carried out. Application of this methodology allowed...
-
Sessile droplet contact angle of water–Al2O3, water–TiO2 and water–Cu nanofluids
PublicationThis work presents measurements of the contact angle of sessile droplets for three nanofluids, i.e. water–Al2O3, water–TiO2 and water–Cu. The plates made of glass, anodized aluminium and stainless steel of different roughness served as substrates. Ultrasonic vibration was used for 30–60 min in order to stabilise the dispersion of the nanoparticles. Nanoparticles were tested at the concentration of 0.01%, 0.1%, and 1% by weight....
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - 3D fracture scan
Open Research DataThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
Ocena możliwości zastosowania stali NV2-4 w budowie statków LPG= Estimation of NV2-4 steel implementation possibilities in LPG ships construction
PublicationPrzedstawiono wyniki badań złączy spawanych ze stali NV2-4 przeznaczonych na konstrukcje naczyń kriogenicznych w statkach LPG. Wykazano przydatność tej stali na tego typu konstrukcje spawane.
-
Electrohydrodynamic flow patterns and collection efficiency in narrow wire-cylinder type electrostatic precipitator
PublicationRecently, narrow electrostatic precipitators (ESPs) have become a subject of interest because of their possible application for the cleaning of the exhaust gases emitted by diesel engines. Diesel engines emit fine particles, which are harmful to human and animal health. There are several methods for decrease particulate emission from a diesel engines, but up to now, these methods are not enough effective or very expensive. Therefore,...
-
A COMPARISON OF WEAR PROPERTIES OF WATER LUBRICATED NBR AND PTFE SLIDING BEARINGS
PublicationThe excessive wear of a journal shaft can be caused by many factors, for example, working conditions (e.g., temperaturę, slip speed, the type of lubricant), pressure, the type of material used on the bearings and shafts and their roughness, as well as contamination remaining in the system. This paper presents the roughness profiles co-operating with a rubber (NBR) and polytetrafluoroethylene (PTFE) bushes. The conditions of cooperation...
-
Electrolytic deposition of reactive element thin films on Crofer 22 APU and evaluation of the resulting high-temperature corrosion protection properties at 700 °C–900 °C
PublicationThis article presents electrolytic deposition of thin Rare Earth (RE) coatings on Crofer 22 APU stainless steel substrates for high temperature applications, such as interconnects in solid oxide cell stacks. The deposition of coatings based on yttrium-, gadolinium-, lanthanum-, and cerium nitrates is discussed. The high temperature corrosion properties of surface-modified steels were examined using thermogravimetry and electrical...
-
Morphology changes in Fe-Cr porous alloys upon high-temperature oxidation quantified by X-ray tomographic microscopy
PublicationThe effect of high-temperature oxidation at 850 C (10 h, 30 h, 100 h) and 900 C (10 h) on porous (30 % porosity) ferritic stainless steel (Fe22Cr) has been investigated using synchrotron tomographic microscopy, which allowed for visualisation, separation and quantitative analysis of the metallic core, closed pores, open pores and oxide scale phase. The same regions within the samples were investigated before and after oxidation...
-
Susceptibility of Cr-Ni-Mn steel to the hydrogen degradation in boiler fuel = Podatnośc stali Cr-Mn-Ni na niszczenie wodorowe w paliwie kotłowym
PublicationStal 34HNM poddana różnym obróbkom cieplnym wykazała skłonność do korozji naprężeniowej w pomiarach ze stałą niską szybkością rozciągania i do zmęczenia korozyjnego niskocyklowego. Mechanizmem zniszczenia była degradacja wodorowa. Możliwe źródła pochłaniania wodoru to: korozja, degradacja węglowodorów z tworzeniem się kwasów organicznych i promotorów wnikania wodoru.
-
Stalowe panele sandwicz - nowe możliwości wynikające z zastosowania spawania laserowego = All steel sandwich panels - new possibilities introduced by laser welding techniques
PublicationW artykule przedstawiono podstawowe dane na temat stalowych paneli typu sandwicz i technik ich wykonywania. Złącze takie charakteryzuje się specyficznymi własnościami, zdecydowanie odmiennymi od klasycznego połączenia spoiną pachwinową, którego cechy wytrzymałościowe i technologiczne są już dobrze opanowane. W podsumowaniu wykazano, że modelowanie jego geometrii musi być prowadzone na znacznie większym poziomie szczegółowości ze...
-
A New Adaptive Method for the Extraction of Steel Design Structures from an Integrated Point Cloud
Open Research DataA new automatic and adaptive algorithm for edge extraction from a random point cloud was developed and presented herein. The proposed algorithm was tested using real measurement data. The developed algorithm is able to realistically reduce the amount of redundant data and correctly extract stable edges representing the geometric structures of a studied...
-
The assessment of metrological properties of segmental orifice based on simulations and experiments
PublicationSegmental orifices are often used to measure flows of heterogeneous mixtures, especially in flow meters in the power industry, for example. The orifice (with module m= 0.25) was installed in a stainless-steel pipe with internal diameter of 50 mm, placed in a hydraulic water system. The research was performed for Reynolds numbers ranging from 9,000 to 17,000. The flow characteristics of this orifice obtained based on simulation...
-
Properties of Barium Cerate Thin Films Formed Using E-Beam Deposition
PublicationThis article focuses on the properties of the BaCeO3 thin films formed by electron-beam vapor deposition and investigates the formation of barium cerates on supports with different thermal expansion coefficients (Stainless Steel, Invar, Glass Sealing, and Inconel substrates) and the influence of the technological parameters on the properties of the formed thin films with an emphasis on the stability of the films. Morphology and...
-
Plate heat exchanger with porous structure for potential use in ORC system
PublicationThe experimental analysis of passive heat transfer intensification in the case of plate heat exchanger has been carried out. The passive intensification was obtained by a modification of the heat transfer surface, which was covered by a metallic porous microlayer. The experiment was accomplished in two stages. In the first stage the commercial stainless steel gasketed plate heat exchanger was investigated, while in the second one...
-
Plate heat exchanger with porous structure for potential use in ORC system
PublicationThe experimental analysis of passive heat transfer intensification in the case of plate heat exchanger has been carried out. The passive intensification was obtained by a modification of the heat transfer surface, which was covered by a metallic porous microlayer. The experiment was accomplished in two stages. In the first stage the commercial stainless steel gasketed plate heat exchanger was investigated, while in the second one...
-
The influence of polymer bearing material and lubricating grooves layout on wear of journal bearings lubricated with contaminated water
PublicationThe goal of the present paper is to investigate wear properties of journal sliding bearing operating in the conditions of contaminated water lubrication. Several bearing materials and bearing sleeve designs (differing in the axial grooves position and their shape) were tested experimentally under typical operating conditions in a dedicated test rig, which was equipped with a lubricating system, enabling lubrication with contaminated...
-
Glass-ceramic joining of Fe22Cr porous alloy to Crofer22APU: interfacial issues and mechanical properties
PublicationThis work deals with the joining of porous Fe22Cr ferritic stainless steel to a dense Crofer22APU plate by using a silica-based, Ba-containing glass-ceramic. The chemical and interfacial stability and the mechanical properties of the joints were evaluated before and after thermal ageing at 700 ◦C for 500hrs. The sintering behaviour of the glass was assessed by using heating stage microscopy (HSM) to study the influence of a porous...
-
Badania jakości docierania stali hartowanej docierakami aktywizowanymi w sposób swobodny = Study of hardened steel lapping quality where lapping tools are activized in a free way
PublicationPrzedstawiono badania jakości docierania stali hartowanej docierakami zbrojonymi w sposób swobodny. Analizowano wpływ podstawowych warunków obróbki na chropowatość powierzchni obrobionej. Wyznaczono zależność parametru Ra od prędkości i czasu docierania oraz nacisku jednostkowego. Analizowano również zanieczyszczenie powierzchni ścierniwem po docieraniu.
-
Corrosion behaviour of low carbon steel in artificial seawater using TP, LP, EIS, Harmonic Analysis (HA) and new method Dynamic Electrochemical Impedance Spectroscopy (DEIS)
PublicationZe względu na istotną rolę technik elektrochemicznych w badaniach procesów korozyjnych są one szeroko stosowane w monitorowaniu korozji. Celem niniejszej pracy jest zgromadzenie rezultatów wyników doświadczalnych uzyskanych różnymi technikami i znalezienie korelacji między nimi. Własności korozyjne stali stopowej (AISI 1026) w sztucznej wodzie morskiej zostały zbadane z wykorzystaniem ekstrapolacji tafelowskiej (TP), polaryzacji...
-
Selected local stability problems of channel section flanges made of aluminium alloys
PublicationThe paper addresses the issue of local buckling of compressed flanges of cold-formed thin-walled channel columns and beams with nonstandard flanges composed of aluminium alloys. The material behaviour follows the Ramberg–Osgood law. It should be noted that the proposed solution may be also applied for other materials, for example: stainless steel, carbon steel. The paper is motivated by an increasing interest in nonstandard cold-formed...
-
EH36 steel for shipbuilding - fracture SEM investigation (plate thicnkness 30mm), a0/W = 0.6
Open Research DataThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...