Abstrakt

The paper presents a method of bending beam test and its importance for evaluation of asphalt mixtures behaviour at low temperatures. Two types of asphalt mixtures: asphalt concrete AC with normal paving grade bitumen and stone mastic asphalt SMA with SBS-modified bitumen were tested. Long-term oven ageing (LTOA) test was also used in the laboratory according to SHRP procedure. The Burgers model was applied and rheological parameters of asphalt mixtures were determined in range of temperature from -10ºC to 10ºC. It has been found that the theoretical Burgers model fits well the experimental data obtained from the creep test. The testing method of bending beam under constant load was relatively simple and easy to use. The paper presents the method of testing, numerical results and analysis of data.

Cytowania

  • 6

    CrossRef

  • 0

    Web of Science

  • 0

    Scopus

Cytuj jako

Pełna treść

pełna treść publikacji nie jest dostępna w portalu

Słowa kluczowe

Informacje szczegółowe

Kategoria:
Aktywność konferencyjna
Typ:
materiały konferencyjne indeksowane w Web of Science
Tytuł wydania:
Advanced Testing and Characterization of Bituminous Materials; Vol. I strony 303 - 312
Język:
angielski
Rok wydania:
2009
Opis bibliograficzny:
Pszczoła M., Judycki J..: Testing of low temperature behaviour of asphalt mixtures in bending creep test, W: Advanced Testing and Characterization of Bituminous Materials; Vol. I, 2009, CRC Press/Balkema,.
DOI:
Cyfrowy identyfikator dokumentu elektronicznego (otwiera się w nowej karcie) 10.1201/9780203092989.ch30
Weryfikacja:
Politechnika Gdańska

wyświetlono 119 razy

Publikacje, które mogą cię zainteresować

Meta Tagi