Ionic conductivity behavior by activated hopping conductivity (AHC) of barium aluminoborosilicate glass–ceramic system designed for SOFC sealing - Publikacja - MOST Wiedzy

Wyszukiwarka

Ionic conductivity behavior by activated hopping conductivity (AHC) of barium aluminoborosilicate glass–ceramic system designed for SOFC sealing

Abstrakt

Non-conducting BaO-B2O3-Al2O3-SiO2 parent glasses designed for solid oxide fuel cell (SOFC) sealing applications were prepared using the melt-quenching technique. The glass formation region was determined according to phase equilibrium relations and was found to be in the composition range 70BaO-(x)Al2O3-(10−x)B2O3-20SiO2 where 3.0 < x < 6.0 wt%. The conductivity values obtained conductivity ranged from 10−5 to 10−10 S/cm at temperatures between 600 and 850 °C. The batch compositions presented a threshold of dc conductivity near 70BaO wt% with a quasi linear behavior with the decrease of the BaO content. Different values of conduction activation energy were observed at temperatures above the glass transition temperature (Tg) (up to 700 °C), which were attributed to the thermal bond-breaking of non-bridging oxygen (NBO) defects. The experimental results of the electrochemical characterization by impedance spectroscopy of glass–ceramic interfaces with yttria-stabilized zirconia (YSZ) acting as solid ionic conductor electrolyte are presented and discussed.

Cytowania

  • 5

    CrossRef

  • 0

    Web of Science

  • 7

    Scopus

Autorzy (6)

Cytuj jako

Pełna treść

pełna treść publikacji nie jest dostępna w portalu

Słowa kluczowe

Informacje szczegółowe

Kategoria:
Publikacja w czasopiśmie
Typ:
artykuł w czasopiśmie wyróżnionym w JCR
Opublikowano w:
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY nr 39, strony 3103 - 3111,
ISSN: 0955-2219
Język:
angielski
Rok wydania:
2019
Opis bibliograficzny:
Da M., Pontuschka W., Bartolomé J., Jasiński P., Karczewski J., Reis S.: Ionic conductivity behavior by activated hopping conductivity (AHC) of barium aluminoborosilicate glass–ceramic system designed for SOFC sealing// JOURNAL OF THE EUROPEAN CERAMIC SOCIETY. -Vol. 39, iss. 10 (2019), s.3103-3111
DOI:
Cyfrowy identyfikator dokumentu elektronicznego (otwiera się w nowej karcie) 10.1016/j.jeurceramsoc.2019.03.027
Weryfikacja:
Politechnika Gdańska

wyświetlono 165 razy

Publikacje, które mogą cię zainteresować

Meta Tagi