Abstrakt

Electrochemical noise data in the presence of pitting corrosion were analyzed. A correlation between the intensity of the observed noise and mass loss of steel electrodes was recognized. The registered noise was decomposed into a set of band limited components using wavelet transform. It has been observed that the standard deviation of the chosen component was more strictly correlated with mass loss of electrodes than the standard deviation of the other components. The frequency band of the chosen component was adequate to the band where energy of transients, typical for pitting corrosion dominated. The measurement results were obtained only for the limited number of electrodes due to a very long time of noise observation.

Cytuj jako

Pełna treść

pełna treść publikacji nie jest dostępna w portalu

Słowa kluczowe

Informacje szczegółowe

Kategoria:
Publikacja w czasopiśmie
Typ:
artykuł w czasopiśmie wyróżnionym w JCR
Opublikowano w:
ELECTROCHEMISTRY COMMUNICATIONS nr 4, wydanie 5, strony 388 - 391,
ISSN: 1388-2481
Język:
angielski
Rok wydania:
2002
Opis bibliograficzny:
Smulko J., Darowicki K., Zieliński A.: Pitting corrosion in steel and electrochemical noise intensity// ELECTROCHEMISTRY COMMUNICATIONS. -Vol. 4, iss. 5 (2002), s.388-391
Weryfikacja:
Politechnika Gdańska

wyświetlono 10 razy

Publikacje, które mogą cię zainteresować

Meta Tagi