Spectral reflectance modeling of ZnO layers made with Atomic Layer Deposition for application in optical fiber Fabry-Perot interferometric sensors

Abstrakt

Suitability of zinc oxide (ZnO) layers grown using Atomic Layer Deposition for operation in optical-fiber extrinsic Fabry-Perot sensors is investigated using a numerical model. Reflectance spectra obtained using the developed model indicate that the application of these layers in optical-fiber extrinsic Fabry-Perot sensors is difficult as it may require a source whose spectrum width is about 300 nm. A series of ZnO layers grown on end faces of SMF-28 fiber were prepared and their reflectance spectra were recorded by an optical spectrum analyser in order to verify the modelling results. The spectra contain a series of peaks not predicted by the model, which is attributed to two-mode propagation in the SMF-28 fiber connecting the ZnO layer with the rest of the measurement system.

Cytowania

  • 2

    CrossRef

  • 2

    Web of Science

  • 0

    Scopus

Pełna treść

pełna treść publikacji nie jest dostępna w portalu

Informacje szczegółowe

Kategoria:
Aktywność konferencyjna
Typ:
materiały konferencyjne indeksowane w Web of Science
Tytuł wydania:
2nd International Symposium on Optics and Biophotonics / Saratov Fall Meeting (SFM) strony 1 - 2
Język:
angielski
Rok wydania:
2015
Opis bibliograficzny:
Wierzba P., Jędrzejewska-Szczerska M..: Spectral reflectance modeling of ZnO layers made with Atomic Layer Deposition for application in optical fiber Fabry-Perot interferometric sensors, W: 2nd International Symposium on Optics and Biophotonics / Saratov Fall Meeting (SFM), 2015, SPIE-INT SOC OPTICAL ENGINEERING, 1000 20TH ST, PO BOX 10, BELLINGHAM, WA 98227-0010 USA,.
DOI:
Cyfrowy identyfikator dokumentu elektronicznego (otwiera się w nowej karcie) 10.1117/12.2179963
Weryfikacja:
Politechnika Gdańska

wyświetlono 15 razy

Publikacje, które mogą cię zainteresować

Meta Tagi