Abstrakt
In this study, the microspheres samples were collected from national power station „Dolna Odra”. In this study, the following materials were used: Portland cement class 32,5R and aggregates of 2-8 and 8-16 fractions and natural sand with a maximum grain size of 2 mm and water. Concrete mixtures were made with microspheres additions of 15%, 25% and 40%. A constant water to binder ratio (w/b) of 0,52 was used throughout the investigation. For each mixture, the distribution of air voids as well as the compressive strength (measured in 2, 28, 56, 90, 180 and 360 day of experiment). In general, the increase in porosity of the concrete with microspheres reduces the compressive strength. The air void content, measured after 28 days, range from 9,7% to 24,3%. With time the microspheres in the environment of cement due to their low surface area (< 500 cm2/g) are slowly reacted with calcium hydroxide to form a gel in the form of hydrated calcium and aluminum silicates.
Autorzy (2)
Cytuj jako
Pełna treść
- Wersja publikacji
- Accepted albo Published Version
- Licencja
-
otwiera się w nowej karcie
Słowa kluczowe
Informacje szczegółowe
- Kategoria:
- Publikacja w czasopiśmie
- Typ:
- artykuły w czasopismach recenzowanych i innych wydawnictwach ciągłych
- Opublikowano w:
-
Materiały Budowlane
strony 50 - 54,
ISSN: 0137-2971 - Język:
- polski
- Rok wydania:
- 2014
- Opis bibliograficzny:
- Haustein E., Quant B.: Wpływ mikrosfer-frakcji odpadów paleniskowych na mikrostrukturę i wybrane właściwości uzytkowe// Materiały Budowlane. -., nr. 1 (2014), s.50-54
- Weryfikacja:
- Politechnika Gdańska
wyświetlono 117 razy
Publikacje, które mogą cię zainteresować
Mechanical properties of two-stage concrete modified by silica fume
- H. Abdelgader,
- R. Fediuk,
- M. Kurpińska
- + 4 autorów