Application of Tensile Creep Test and Viscoelastic Method to the Analysis of Thermal Stresses at Low Temperatures

Abstract

The paper presents the viscoelastic method of thermal stresses calculation with utilization of results from tensile creep test (TCT) at a temperature range from −20 to +20 °C (in the case of asphalt concrete with styrene-butadiene-styrene (SBS) polymer-modified bitumen from −30 to +20 °C). Two types of neat road bitumen 35/50 and 50/70 and polymer SBS-modified bitumen 45/80–55 were tested for tensile creep properties at low temperatures. On the basis of laboratory results, the master curves of stiffness modulus were developed using Richards model. For calculation of thermal stresses, Burgers’ rheological model was used, and rheological parameters describing elastic and viscous properties of the asphalt mixtures were determined. Then the viscoelastic method was applied based on the assumption that asphalt layer is made of a linear viscoelastic material that responses under load at a constant temperature and can be mathematically described by the Burgers model. It was concluded that the laboratory TCT test provides reliable results for thermal stress calculations, and that the viscoelastic method of thermal stresses calculation allow to model different rates of temperature and provides good foundation for the calculation of the thermal stresses generated by the real winter thermal cycles.

Citations

  • 0

    CrossRef

  • 0

    Web of Science

  • 0

    Scopus

Cite as

Full text

full text is not available in portal

Keywords

Details

Category:
Monographic publication
Type:
rozdział, artykuł w książce - dziele zbiorowym /podręczniku w języku o zasięgu międzynarodowym
Language:
English
Publication year:
2024
Bibliographic description:
Pszczoła M., Jaczewski M.: Application of Tensile Creep Test and Viscoelastic Method to the Analysis of Thermal Stresses at Low Temperatures// 14th International Conference on Asphalt Pavements ISAP2024 Montreal/ : , 2024, s.747-752
DOI:
Digital Object Identifier (open in new tab) 10.1007/978-3-031-67252-1_123
Sources of funding:
  • Statutory activity/subsidy
Verified by:
Gdańsk University of Technology

seen 17 times

Recommended for you

Meta Tags