Abstract
Citations
-
1 1
CrossRef
-
0
Web of Science
-
1 2
Scopus
Authors (2)
Cite as
Full text
full text is not available in portal
Details
- Category:
- Magazine publication
- Type:
- Magazine publication
- Published in:
-
JOURNAL OF SOLID STATE ELECTROCHEMISTRY
no. 13,
edition 11,
pages 1653 - 1657,
ISSN: 1432-8488 - ISSN:
- 1432-8488
- Publication year:
- 2009
- DOI:
- Digital Object Identifier (open in new tab) 10.1007/s10008-008-0759-0
- Verified by:
- No verification
seen 39 times