Glass-ceramic sealants and steel interconnects: accelerated interfacial stability and reactivity tests at high temperature
Abstract
High-temperature reactions between glass-ceramic sealants and Fe-Cr alloy interconnects may lead to the formation of undesirable phases, and consequently degradation of solid oxide fuel/electrolyser devices. In this work, three different glass-ceramic sealants (Na-containing, Ba-containing, Sr-containing compositions) and Fe22Cr stainless steel powders (raw and pre-oxidised) are considered in order to test their chemical reactivity at 750°C and 850 °C for 500 h in static air. The novelty of this approach is related to the use of powder mixtures instead of studying the reactivity on planar interfaces, which allows a better evaluation the materials’ reactivity. Oxidation tests indicate that the Sr-containing glass-ceramic/steel couple is the least reactive among the aged samples. For the Ba-containing samples, the formation of an undesirable phase of BaCrO4 is observed by diffractometry and photoelectron spectroscopy analyses. The present research explores, for the first time, the effects of exposing the high surface area of the alloy powder and glass-ceramic sealant interface, assessed by oxidation testing and microstructural analysis. The results show that by using mixed powders with large interface surface areas, degradation of the materials can be observed after relatively short times, allowing accelerated screening of the reactivity of materials, and thus their further development.
Citations
-
4
CrossRef
-
0
Web of Science
-
8
Scopus
Authors (10)
Cite as
Full text
- Publication version
- Accepted or Published Version
- DOI:
- Digital Object Identifier (open in new tab) 10.1016/j.matdes.2021.110259
- License
- open in new tab
Keywords
Details
- Category:
- Articles
- Type:
- artykuły w czasopismach
- Published in:
-
MATERIALS & DESIGN
no. 212,
ISSN: 0264-1275 - Language:
- English
- Publication year:
- 2021
- Bibliographic description:
- Drewniak A., Koszelow D., Błaszczak P., Górnicka K., Jurak K., Javed H., Sabato A. G., Jasiński P., Molin S., Smeacetto F.: Glass-ceramic sealants and steel interconnects: accelerated interfacial stability and reactivity tests at high temperature// MATERIALS & DESIGN -Vol. 212, (2021), s.110259-
- DOI:
- Digital Object Identifier (open in new tab) 10.1016/j.matdes.2021.110259
- Sources of funding:
-
- Project Corrosion of Porous Alloys
- Verified by:
- Gdańsk University of Technology
seen 146 times
Recommended for you
Glass-ceramic joining of Fe22Cr porous alloy to Crofer22APU: interfacial issues and mechanical properties
- F. D'Isanto,
- M. Salvo,
- S. Molin
- + 5 authors
X-Ray Computer Tomography Study of Degradation of the Zircaloy-2 Tubes Oxidized at High Temperatures
- B. Trybuś,
- J. Olive,
- N. Lenoir
- + 1 authors
Wear Resistance Enhancement of Al6061 Alloy Surface Layer by Laser Dispersed Carbide Powders
- R. Jendrzejewski,
- J. Łubiński,
- G. Śliwiński
Dissimilar autogenous TIG joint of Alloy 617 and AISI 304H steel for AUSC application
- S. Sirohi,
- A. Kumar,
- S. M. Pandey
- + 4 authors