Chemical oxygen surface exchange coefficient (k*) of the SrxTi0.30Fe0.70O3 (x=0.90, 0.95 and 1.00) at different temperatures
Description
In this dataset are presented k* values designated based on the analysis of the electrical conductivity relaxation (ECR) mesurement of the SrxTi0.30Fe0.70O3 (x=0.90, 0.95, 1.00) materials. The applied temperatures were 800 °C, 750 °C, 700 °C, 650 °C, and 600 °C. Studies were performed in a small tube furnace (internal diameter ~20 mm) with 64 cm3 gas volume. During the four-point single frequency electrochemical impedance spectroscopy measurement (1 Hz), the oxygen partial pressures were changed from 20% O2 to 10% O2 and the reverse.
k* was designated for both cases incorporation and removal of oxygen.
Dataset file
k vs temp.xlsx
8.8 kB,
S3 ETag
7d0fa5e023fabd22bf732ddde309f139-1,
downloads: 3
The file hash is calculated from the formula
Example script for calculation:
https://github.com/antespi/s3md5
hexmd5(md5(part1)+md5(part2)+...)-{parts_count}
where a single part of the file is 512 MB in size.Example script for calculation:
https://github.com/antespi/s3md5
File details
- License:
-
open in new tabCC BYAttribution
Details
- Year of publication:
- 2022
- Verification date:
- 2024-11-27
- Dataset language:
- English
- Fields of science:
-
- Automation, electronic and electrical engineering (Engineering and Technology)
- materials engineering (Engineering and Technology)
- DOI:
- DOI ID 10.34808/jq6v-bj64 open in new tab
- Funding:
- Series:
- Verified by:
- Gdańsk University of Technology
Keywords
- perovskite
- oxygen electrode
- strontium doped titanates
- nonstoichiometry
- oxygen reduction
- oxygen evolution
Cite as