Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #24 - #25.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #24 (upper, rotating), #25 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #28 - #29.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #28 (upper, rotating), #29 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #30 - #31.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #30 (upper, rotating), #31 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #20 - #21.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #20 (upper, rotating), #21 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #22 - #23.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #22 (upper, rotating), #23 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #28 - #29.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #28 (upper, rotating), #29 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #26 - #27.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #26 (upper, rotating), #27 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 4-8h.
Open Research DataWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 4-8h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 0-4h.
Open Research DataWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 0 - 4h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 0-4h. High frequency burst recording.
Open Research DataWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. High frequency burst recording.Running time: 0 - 4h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21,...