Research fields
-
Barrett-Joyner-Halenda (BJH) and Brunauer-Emmett-Teller (BET) analysis of wood and straw based biochars
Open Research DataThis data set includes the BJH and BET analysis results for straw and wood chips-based biochars generated at 450 Celsius degrees.
-
Structural and luminescence properties of B2O3-Bi2O3+10AlF3 glasses doped with Eu3+/Dy3+ ions
Open Research DataThe attached data contains the results of measurements of B2O3-Bi2O3 and B2O3-Bi2O3+10AlF3 glasses doped with Eu3+ and Dy3+ ions in different molar ratios. Glasses were synthesized by the melt quenching technique. On their basis, the structural, optical, and luminescence properties of synthesized samples were characterized. The dataset includes XRD,...
-
TG and DTG profiles for plastics: LDPE, HDPE, PP, PD and PET
Open Research DataThe dataset includes:
-
Influence of controlled crystallization and SrF2 content on the structure and properties of Eu3+ doped phosphate glasses
Open Research DataThe attached data contains the results of measurements of phosphate glasses and glass-ceramics doped with Eu. On their basis, the new material was characterized and the influence of the SrF2 addition on the glass structure was determined. In addition, the influence of the SrF2 content and controlled crystallization on the luminescent properties of Eu3+...
-
XRD, DTA and luminescence measurements of B2O3-Bi2O3-AlF3 glasses doped with Eu3+, Tb3+ and Tm3+ ions
Open Research DataThe DataSet contains the XRD,DTA and luminescence measurements for the B2O3-Bi2O3-AlF3 glass system. Samples were prepared by the conventional melt quenching technique. Starting materials were melted in porcelain crucibles at 950 oC for 20 min. XRD and DTA data were collected for 50B2O3-50Bi2O3,45B2O3-45Bi2O3+10AlF3 and 40B2O3-40Bi2O3+20AlF3 glasses....
-
Luminescence and FTIR measurements of B2O3-Bi2O3-SrF2 glass and glass-ceramics doped with Eu3+ ions
Open Research DataLuminescence and FTIR measurements of B2O3-Bi2O3-xSrF2+2Eu (x=10,20) glass and glass-ceramics. The emission and excitation spectra of the samples depend on the composition and annealing time.