Brunauer-Emmett-Teller (BET) surface analysis of titanium dioxide (TiO2) and silicon dioxide (SiO2) used for coating of expanded polystyrene spheres (EPS)
Description
Data refer to the results of BET surface area of TiO2 and SiO2 powders used for coating of expanded polystyrene spheres. The detailed measurement and equipment data was described in readme BET.txt file.
TiO2 was treated firstly in autoclave at 150 C degrees for 1h, then was further heat treated in Ar at 400 C degrees. As a raw material TiO2 was used, which was a semiproduct from the industrial production of titania white by sulphur method. The raw material was mostly amorphous and contained some nuclei of rutile and sulphur species. SiO2 was obtained via modified Strober method.
Dataset file
BET.zip
32.7 kB,
S3 ETag
db97efc2a4ce26c087c38635a0669243-1,
downloads: 35
The file hash is calculated from the formula
Example script for calculation:
https://github.com/antespi/s3md5
hexmd5(md5(part1)+md5(part2)+...)-{parts_count}
where a single part of the file is 512 MB in size.Example script for calculation:
https://github.com/antespi/s3md5
File details
- License:
-
open in new tabCC BYAttribution
Details
- Year of publication:
- 2024
- Related location:
- Szczecin, województwo zachodniopomorskie, Polska (53° 25′ 29″ N, 14° 32′ 8″ E)
- Verification date:
- 2024-02-12
- Creation date:
- 2023
- Dataset language:
- English
- Fields of science:
-
- chemical engineering (Engineering and Technology)
- materials engineering (Engineering and Technology)
- DOI:
- DOI ID 10.34808/7k25-jw97 open in new tab
- Funding:
- Verified by:
- West Pomeranian University of Technology in Szczecin
Keywords
- titanium dioxide
- silicon dioxide
- Brunauer-Emmett-Teller (BET) surface analysis
- expanded polystyrene spheres
References
- publication Enhanced Ethylene Removal in a Fluidized Bed Photoreactor with Polystyrene as a Novel Bed
Cite as
Authors
seen 72 times