Mechanical properties of single V2O5 nanocrystal - nanoindentation measurement in control of the max-depth
Description
The DataSet contains the nanoindentation curves (indentation force Fn vs penetrationPd) for a single V2O5 nanocrystal supported on a substrate. The measurements were performed in control of the maximum depth of Berkovich indenter penetration: 60, 70, and 100 nm.
Nanoindentation curves were collected on a Nanoidenter TTX-NHT2 CSM. The details about measurements are included in each .text file.
Dataset file
max depth.zip
211.5 kB,
S3 ETag
d9d77519743d631be9eabb2963e75107-1,
downloads: 51
The file hash is calculated from the formula
Example script for calculation:
https://github.com/antespi/s3md5
hexmd5(md5(part1)+md5(part2)+...)-{parts_count}
where a single part of the file is 512 MB in size.Example script for calculation:
https://github.com/antespi/s3md5
File details
- License:
-
open in new tab
CC BYAttribution - Raw data:
- Data contained in dataset was not processed.
Details
- Year of publication:
- 2021
- Verification date:
- 2021-06-21
- Dataset language:
- English
- Fields of science:
-
- materials engineering (Engineering and Technology)
- DOI:
- DOI ID 10.34808/8dze-b590 open in new tab