Description

The DataSet contains the nanoindentation curves (indentation force Fn vs penetrationPd) for a single V2O5 nanocrystal supported on a substrate. The measurements were performed in control of the maximum load of  Berkovich indenter force from 2 to 50 mN. 

Nanoindentation curves were collected on a Nanoidenter TTX-NHT2 CSM. The details about measurements are included in each .text file.

Dataset file

max load.zip
212.6 kB, S3 ETag 81af174058f4e89dbf7dd76234bd2415-1, downloads: 54
The file hash is calculated from the formula
hexmd5(md5(part1)+md5(part2)+...)-{parts_count} where a single part of the file is 512 MB in size.

Example script for calculation:
https://github.com/antespi/s3md5
download file max load.zip

File details

License:
Creative Commons: by 4.0 open in new tab
CC BY
Attribution
Raw data:
Data contained in dataset was not processed.

Details

Year of publication:
2021
Verification date:
2021-06-21
Dataset language:
English
Fields of science:
  • materials engineering (Engineering and Technology)
DOI:
DOI ID 10.34808/jprz-7a38 open in new tab
Series:
Verified by:
Gdańsk University of Technology

Keywords

References

Cite as

seen 111 times