Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K06
Description
Optical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.
Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.
Linear reciprocating motion.
Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.
Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. Wear mark examination at each intermission between test segments.
Specimen set K06
Dataset file
K06.rar
8.4 MB,
S3 ETag
809171bf3ed2906c547f34f1ccde6735-1,
downloads: 44
The file hash is calculated from the formula
Example script for calculation:
https://github.com/antespi/s3md5
hexmd5(md5(part1)+md5(part2)+...)-{parts_count}
where a single part of the file is 512 MB in size.Example script for calculation:
https://github.com/antespi/s3md5
File details
- License:
-
open in new tabCC BY-NCNon-commercial
- Raw data:
- Data contained in dataset was not processed.
Details
- Year of publication:
- 2021
- Verification date:
- 2021-05-30
- Dataset language:
- English
- Fields of science:
-
- mechanical engineering (Engineering and Technology)
- materials engineering (Engineering and Technology)
- DOI:
- DOI ID 10.34808/s7tc-bp12 open in new tab
- Series:
- Verified by:
- Gdańsk University of Technology
Keywords
Cite as
Authors
seen 84 times