Determination of pitting corrosion stage of stainless steel by galvanodynamic impedance spectroscopy
Abstract
This paper investigates the methodology for differentiation of multistep process of pitting corrosion of AISI 304 stainless steel in the environment of iron (III) chloride. Measurements were performed using Galvanodynamic Electrochemical Impedance Spectroscopy (GDEIS). Application of this methodology allowed monitoring of natural corrosion process without external current (IDC = 0A) nor potential perturbation of the system. Applied sinusoidal AC current does not influence significantly registered DC potential. Analysis confirms that it is possible to distinguish all stages of pitting corrosion: passive state, metastable state, initiation of pitting, active pitting corrosion state. Characteristic potential oscillations related with pitting corrosion were detected. Research shows that GDEIS method can be with success utilized in the monitoring of pitting corrosion.
Citations
-
2 8
CrossRef
-
0
Web of Science
-
3 0
Scopus
Authors (4)
Cite as
Full text
full text is not available in portal
Keywords
Details
- Category:
- Articles
- Type:
- artykuł w czasopiśmie wyróżnionym w JCR
- Published in:
-
ELECTROCHIMICA ACTA
no. 253,
pages 403 - 412,
ISSN: 0013-4686 - Language:
- English
- Publication year:
- 2017
- Bibliographic description:
- Orlikowski J., Jażdżewska A., Mazur R., Darowicki K.: Determination of pitting corrosion stage of stainless steel by galvanodynamic impedance spectroscopy// ELECTROCHIMICA ACTA. -Vol. 253, (2017), s.403-412
- DOI:
- Digital Object Identifier (open in new tab) 10.1016/j.electacta.2017.09.047
- Verified by:
- Gdańsk University of Technology
seen 189 times
Recommended for you
Corrosion Monitoring in Petroleum Installations—Practical Analysis of the Methods
- J. Orlikowski,
- A. Jazdzewska,
- I. Łuksa
- + 2 authors