Abstract
The paper presents the results of the pitting resistance investigations of selected stainless steels in the chloride environment and the simultaneous impact of erosive factors using the cyclic polarization technique. Additionally, using electrochemical techniques, ie: electrochemical impedance spectroscopy (EIS) and measurement of corrosion potential, the behavior of the passive layer of selected stainless steels in the environment of chlorides and erosion was examined. On the basis of the obtained results, the resistance of stainless steels 1.4301 and 1.4404 was found, both on the effect of chloride ions and erosive factors in the studied systems. Both tested steels are susceptible to pitting corrosion. It was found that a good measure of erosive impact on stainless steel is both impedance spectrum analysis and continuous monitoring of the corrosion potential of steel.
Citations
-
0
CrossRef
-
0
Web of Science
-
0
Scopus
Authors (2)
Cite as
Full text
- Publication version
- Accepted or Published Version
- License
-
open in new tab
Keywords
Details
- Category:
- Articles
- Type:
- artykuły w czasopismach
- Published in:
-
ARCHIVES OF METALLURGY AND MATERIALS
no. 64,
pages 1627 - 1632,
ISSN: 1733-3490 - Language:
- English
- Publication year:
- 2019
- Bibliographic description:
- Krakowiak S., Kierepa S.: The Impact of Crushed Rock Spoil on Pitting Corrosion of Selected Stainless Steel// ARCHIVES OF METALLURGY AND MATERIALS -Vol. 64,iss. 4 (2019), s.1627-1632
- DOI:
- Digital Object Identifier (open in new tab) 10.24425/amm.2019.130136
- Verified by:
- Gdańsk University of Technology
seen 156 times
Recommended for you
Hydrogen Damage in Superaustenitic 904L Stainless Steels
- J. Michalska,
- B. Chmiela,
- J. Łabanowski
- + 1 authors
An investigation of microstructural basis for corrosion behavior of Al-CNT composites fabricated by SPS
- O. Ekhlasiosgouei,
- R. Ebrahimi,
- M. Hasheminiasari
- + 1 authors
Electrochemical investigations on corosivity of de-icing liquids for railway infrastructure
- K. Brzóska,
- D. Sikorska,
- S. Krakowiak