The SEM micrographs of the synergistic action between cavitation erosion and pitting corrosion on stainless steel 304

Description

The dataset contains Scanning Electron Micrographs of stainless steel AISI304 samples made after cavitation erosion-corrosion exposure using a vibratory transducer (in accordance with ASTM G32). The micrographs compare the topography of samples subjected to either cavitation erosion (in deionized water), pitting corrosion (in 8% FeCl3 solution, without cavitation) or cavitation erosion-corrosion (cavitation erosion in 8% FeCl3 solution). The experiment lasted between 5 and 240 min, labeled accordingly, with cyclic cavitation exposure in on/off cycles 30s:30s. The samples were mounted directly underneath the ultrasonic transducer.

Dataset file

cav_corr.rar
298.5 MB, S3 ETag a81e632b84cf0eff1cbbbfd8ee410a09-1, downloads: 53
The file hash is calculated from the formula
hexmd5(md5(part1)+md5(part2)+...)-{parts_count} where a single part of the file is 512 MB in size.

Example script for calculation:
https://github.com/antespi/s3md5

File details

License:
Creative Commons: by 4.0 open in new tab
CC BY
Attribution
Raw data:
Data contained in dataset was not processed.

Details

Year of publication:
2020
Verification date:
2020-12-17
Creation date:
2013
Dataset language:
English
Fields of science:
  • materials engineering (Engineering and Technology)
DOI:
DOI ID 10.34808/805a-h462 open in new tab
Verified by:
Gdańsk University of Technology

Keywords

Cite as

seen 108 times