Microstructure and mechanical properties of laser surface-treated Ti13nb13zr alloy with MWCNTs coatings
PublicationLaser surface modification of titanium alloys is one of the main methods of improving the properties of titanium alloys used in implantology. This study investigates the microstructural morphology of a laser-modified surface layer on a Ti13Nb13Zr alloy with and without a carbon nanotube coating deposited by electrophoretic deposition. Laser modification was performed for samples with and without carbon nanotube coating for two...
-
Effect of selective laser treatment on initiation of fatigue crack in the main part of an undercarriage drag strut
PublicationThis paper presents the results of material characterization and a fatigue test conducted for a laser-re-melted drag strut used in an aircraft landing gear. The drag strut was re-melted with a CO2 laser beam. Eight re-melted paths were made in the form of spiral lines along the axis of the drag strut. Next, the drag strut was subjected to variable loads on a testing machine simulating loads occurring when an aircraft lands. The...