Open Research Data - Exsolution
Filters
total: 18
Open Research Data Series
-
The EDS elemental maps of reduced LSCNT (SEM)
Open Research DataThe dataset includes elemental maps of La, Ce, Ti, O, Sr, Ni in La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s produced using Pechini method sintered at 1200oC under air atmosphere and reduced at 900 for 12 h in wet H2.
-
The TEC measurement of LSCNT (dilatometry) in air
Open Research DataThe dataset includes dilatometry results for La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s measured in air from 100 to 800C using Netzsch DIL 402 PC.
-
The XRD diffraction patterns of reduced LSCNT prepared using two methods and two sintering temperatures
Open Research DataThe dataset includes XRD diffraction patterns of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s produced using two methods, namely organic (citrate assisted) and Pechini sintered at 1000 or 1200oC under air atmosphere and reduced at 900 for 12 h in wet H2.
-
FTIR spectra of SOFC with LSCNT layer fueled by biogas mixture at 750 C (pure)
Open Research DataThe dataset contains the FTIR spectra collected during the electrical measurements DIR-SOFC with LSCNT layer. The SOFC was reduced at 800degC in H2 prior to mesurements. The spectra were collected every 10 min.
-
Electrical performance measurement of reference and SOFC with LSCNT layer fueled by H2 and 20ppm H2S/biogas mixture at 750 C - cyclic measurements (12h per cycle)
Open Research DataThe dataset contains the electrical IV measurements collected during the cyclic measurements of H2S poisoning in DIR-SOFC with/-out LSCNT layer. The H2S poisoning and H2 regenrating cycles were 12 h each. The spectra were collected every 10 min.
-
FTIR spectra of SOFC with LSCNT layer fueled by H2 and 20ppm H2S/biogas mixture at 750 C - cyclic measurements (12h per cycle)
Open Research DataThe dataset contains the FTIR spectra collected during the cyclic measurements of H2S poisoning in DIR-SOFC with LSCNT layer. The H2S poisoning and H2 regenrating cycles were 12 h each. The spectra were collected every 10 min.
-
FTIR spectra of reference SOFC fueled by H2 and 20ppm H2S/biogas mixture at 750 C - cyclic measurements (12h per cycle)
Open Research DataThe dataset contains the FTIR spectra collected during the cyclic measurements of H2S poisoning in DIR-SOFC without LSCNT layer. The H2S poisoning and H2 regenrating cycles were 12 h each. The spectra were collected every 10 min.
-
Electrical power measurement of reference SOFC fueled by biogas mixture at 750 C
Open Research DataThe dataset contains the electrical measurements of IV curves for SOFC without La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s layer working under biogas and H2 feeding stream. The SOFC was reduced at 900C and conditioned for 12 h under H2 prior the measurements. The measurements were performed using Gamry potentiostat/galvanostat
-
Electrical power measurement of LSCNT modified SOFC fueled by biogas mixture at 750 C
Open Research DataThe dataset contains the electrical measurements of IV curves for SOFC with La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s layer working under biogas and H2 feeding stream. The SOFC was reduced at 900C and conditioned for 12 h under H2 prior the measurements. The measurements were performed using Gamry potentiostat/galvanostat
-
Change of exhaust gases concentration for LSCNT modified SOFC fueled by biogas mixture at 750 C
Open Research DataThe dataset changes of exhaust gases concentrations (CH4,CO,CO2,H2) over working time for SOFC with La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s layer. Concentrations were calculated based on the FTIR measurements and calibration files presented in coupled dataset.
-
The XRD diffraction patterns of LSCNT of different A site nonstoichiometry
Open Research DataThe dataset includes XRD diffraction patterns of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s and La0.3Sr0.6Ce0.1Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The SEM images of LSCNT reduced at 1000 degrees C under H2
Open Research DataThe dataset includes SEM images of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h and reduced at 1000oC under H2 for 10 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The SEM images of LSCNT reduced at 900 degrees C under H2
Open Research DataThe dataset includes SEM image of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h and reduced at 900oC under H2 for 10 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The SEM images of LSCNT reduced at 800 degrees C under H2
Open Research DataThe dataset includes SEM images of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h and reduced at 800oC under H2 for 10 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The SEM images of LSCNT sintered at 1200 degrees C in air
Open Research DataThe dataset includes SEM images of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h. Samples were produced using aqueous soft chemistry methods (Pechini). The grain structure can be seen on higher resolution image.
-
Change of exhaust gases concentration for reference SOFC and SOFC with LSCNT layer fueled by biogas mixture at 750 C
Open Research DataThe dataset changes of exhaust gases concentrations (CH4,CO,CO2,H2) over working time for SOFC with La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s layer as well as reference SOFEC (unmodified). Concentrations were calculated based on the FTIR measurements and calibration curves presented in different dataset. Longterm measurements of SOFC were performed using in-house...
-
The XPS spectra of LSCNT sintered at 1200C
Open Research DataThe dataset includes XPS spectra of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at various temperatures under air atmosphere for 12 h. Samples were produced using aqueous soft chemistry methods (Pechini). The XPS spectra were collected for all species.
-
The XRD diffraction patterns of LSCNT sintered at various temperatures
Open Research DataThe dataset includes XRD diffraction patterns of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at various temperatures under air atmosphere for 12 h. Samples were produced using aqueous soft chemistry methods (Pechini).