Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K04 - Open Research Data - Bridge of Knowledge

Search

Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K04

Description

Optical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.
Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.
Linear reciprocating motion.
Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.
Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. Wear mark examination at each intermission between test segments.
Specimen set K04

 

Dataset file

K04.rar
16.4 MB, S3 ETag 08c210d360c0c8afd4e3d3dcd66d1d98-1, downloads: 52
The file hash is calculated from the formula
hexmd5(md5(part1)+md5(part2)+...)-{parts_count} where a single part of the file is 512 MB in size.

Example script for calculation:
https://github.com/antespi/s3md5

File details

License:
Creative Commons: by-nc 4.0 open in new tab
CC BY-NC
Non-commercial
Raw data:
Data contained in dataset was not processed.

Details

Year of publication:
2021
Verification date:
2021-05-30
Dataset language:
English
Fields of science:
  • mechanical engineering (Engineering and Technology)
  • materials engineering (Engineering and Technology)
DOI:
DOI ID 10.34808/zhb9-n881 open in new tab
Series:
Verified by:
Gdańsk University of Technology

Keywords

Cite as

seen 97 times