Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K04 - Open Research Data - MOST Wiedzy

Wyszukiwarka

Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K04

Opis

Optical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.
Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.
Linear reciprocating motion.
Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.
Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. Wear mark examination at each intermission between test segments.
Specimen set K04

 

Plik z danymi badawczymi

K04.rar
16.4 MB, S3 ETag 08c210d360c0c8afd4e3d3dcd66d1d98-1, pobrań: 55
Hash pliku liczony jest ze wzoru
hexmd5(md5(part1)+md5(part2)+...)-{parts_count} gdzie pojedyncza część pliku jest wielkości 512 MB

Przykładowy skrypt do wyliczenia:
https://github.com/antespi/s3md5

Informacje szczegółowe o pliku

Licencja:
Creative Commons: by-nc 4.0 otwiera się w nowej karcie
CC BY-NC
Użycie niekomercyjne
Dane surowe:
Dane zawarte w datasecie nie zostały w żaden sposób przetworzone.

Informacje szczegółowe

Rok publikacji:
2021
Data zatwierdzenia:
2021-05-30
Język danych badawczych:
angielski
Dyscypliny:
  • inżynieria mechaniczna (Dziedzina nauk inżynieryjno-technicznych)
  • inżynieria materiałowa (Dziedzina nauk inżynieryjno-technicznych)
DOI:
Identyfikator DOI 10.34808/zhb9-n881 otwiera się w nowej karcie
Seria:
Weryfikacja:
Politechnika Gdańska

Słowa kluczowe

Cytuj jako

wyświetlono 103 razy