Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K01
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate folders).Specimen...
-
Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K04
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate folders).Specimen...
-
Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K05
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate folders).Specimen...
-
Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K03
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate folders).Specimen...
-
Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K06
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate...
-
Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - PARAFFIN OIL. Specim. set K08
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: PARAFFIN OIL. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate...
-
Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K07
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate...
-
Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K02
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K05
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K03
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K04
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K01
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - PARAFFIN OIL. Specim. set K08
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: PARAFFIN OIL. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30,...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K02
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15,...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K06
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15,...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K07
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15,...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #24 - #25.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #24 (upper, rotating), #25 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #28 - #29.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #28 (upper, rotating), #29 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #30 - #31.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #30 (upper, rotating), #31 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #20 - #21.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #20 (upper, rotating), #21 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #22 - #23.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #22 (upper, rotating), #23 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #28 - #29.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #28 (upper, rotating), #29 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #26 - #27.
Open Research DataSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #26 (upper, rotating), #27 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - PARAFFIN OIL. Specim. set K09 - full run
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: PARAFFIN OIL. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate...
-
Wear in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - PARAFFIN OIL. Specim. set K09 - pre-run (10s)
Open Research DataFriction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: PARAFFIN OIL. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. (stored in separate...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - PARAFFIN OIL. Specim. set K09A - full-run
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: PARAFFIN OIL. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30,...
-
VIbration monitoring in reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - PARAFFIN OIL. Specim. set K09 - pre-run
Open Research DataVIbration monitoring in reciprocating siding friction tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: PARAFFIN OIL. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.Running time: progressive increments of 10, 15, 30,...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K04
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K05
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K03
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K01
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K07
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K06
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - PARAFFIN OIL. Specim. set K08
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: PARAFFIN OIL. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig:...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K02
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - PARAFFIN OIL. Specim. set K09
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: PARAFFIN OIL. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig:...
-
Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). Lubricant - DISTILLED WATER. Specim. set K06
Open Research DataOptical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.Linear reciprocating motion.Lubrication: DISTILLED WATER. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 4-8h.
Open Research DataWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 4-8h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 0-4h.
Open Research DataWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 0 - 4h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 0-4h. High frequency burst recording.
Open Research DataWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. High frequency burst recording.Running time: 0 - 4h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21,...
-
SiC coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #B37/#A35
Open Research DataWear tests in sliding friction of SiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, SiC over SiC . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 3 min.Secimen...
-
TiC coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #A39/#B41
Open Research DataWear tests in sliding friction of TiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiC over TiC . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 3 min.Secimen...
-
SiC coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #A35/#B37
Open Research DataWear tests in sliding friction of SiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, SiC over SiC . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 3 min.Secimen...
-
Atomic force microscopy images of copper electrical contacts wear under the influence of friction
Open Research DataMeasurement of wear of copper electrical contacts under the influence of friction. Imaging in contact mode in the variant of scanning spreading resistance microscopy. Additionally, there are spectroscopic current-voltage curves showing local changes in electrical conductivity. NTEGRA Prima (NT-MDT) device. Probe NSG 01Pt.
-
TiN coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #B48/#A45
Open Research DataWear tests in sliding friction of TiN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiN over TiN . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 12 min....
-
TiC coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #B41/#A39
Open Research DataWear tests in sliding friction of TiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiC over TiC . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 9 min....
-
CrN coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #A23/#B22
Open Research DataWear tests in sliding friction of CrN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, CrN over CrN . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 12 min. The...
-
TiC coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #B39/#A41
Open Research DataWear tests in sliding friction of TiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiC over TiC . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 3 min. The test...
-
SiC coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #B34/#A33
Open Research DataWear tests in sliding friction of SiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, SiC over SiC. Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 3 min. The test...
-
TiN coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #A45/#B48
Open Research DataWear tests in sliding friction of TiN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiN over TiN . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 12 min....