Search results for: cathode material
-
SEM micrographs of V2O5 nanorods as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 nanorods as cathode materials before and after the galvanostatic charge/discharge curves.
-
SEM micrographs of V2O5 nanocrystals as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 nanocrystals as cathode materials before and after the galvanostatic charge/discharge curves.
-
Cycling performances of the V2O5 nanorods as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the next one hundred galvanostatic charge/discharge curves of the V2O5 nanorods obtained by the sol-gel method. The battery tests of the samples were performed using the Atlas-Sollich 0961 (Atlas-Sollich, Poland) with C/5 and 2C current densities in the voltage range between 2.0 V and 4.0 V vs. Li/Li+. Here 1C is 294 mAh g-1. The...
-
Cycling performances of the V2O5 nanocrystals as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the next one hundred galvanostatic charge/discharge curves of the V2O5 nanocrystals obtained by the sol-gel method. The battery tests of the samples were performed using the Atlas-Sollich 0961 (Atlas-Sollich, Poland) with C/5 and 2C current densities in the voltage range between 2.0 V and 4.0 V vs. Li/Li+. Here 1C is 294 mAh g-1. ...
-
Cycling performances of the V2O5 nanostructures as cathode material in Na-ion batteries
Open Research DataThe DataSet contains the next one hundred galvanostatic charge/discharge curves of the V2O5 nanostructures with different morphology obtained by the sol-gel method. The battery tests of the samples were performed using the Atlas-Sollich 0961 (Atlas-Sollich, Poland) with C/5 current densities in the voltage range between 2.0 V and 4.0 V vs. Li/Li+. Here...
-
Rate performance of the V2O5 nanocrystals as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the galvanostatic charge/discharge curves of the V2O5 nanocrystals obtained by the sol-gel method. The battery tests of the samples were performed using the Atlas-Sollich 0961 (Atlas-Sollich, Poland) with different current densities in the voltage range between 2.0 V and 4.0 V vs. Li/Li+. Here 1C is 294 mAh g-1.
-
Rate performance of the V2O5 nanorods as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the galvanostatic charge/discharge curves of the V2O5 nanorods obtained by the sol-gel method. The battery tests of the samples were performed using the Atlas-Sollich 0961 (Atlas-Sollich, Poland) with different current densities in the voltage range between 2.0 V and 4.0 V vs. Li/Li+. Here 1C is 294 mAh g-1.
-
Rate performance of (NH4)2V10O25·8H2O as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the galvanostatic charge/discharge curves of the ammonium vanadate nanostructures obtained by the hydrothermal method under an initial pressure of 50 bar ((NH4)2V10O25·8H2O). The battery tests of the samples were performed using the ATLAS 0961 MBI multichannel battery testing system with different current densities in the voltage...
-
Rate performance of mixture (NH4)2V6O16 and (NH4)2V10O25·8H2O as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the galvanostatic charge/discharge curves of the ammonium vanadate nanostructures obtained by the hydrothermal method without initial pressure (mixture (NH4)2V6O16 and (NH4)2V10O25·8H2O). The battery tests of the samples were performed using the ATLAS 0961 MBI multichannel battery testing system with different current densities...
-
SEM micrographs of Ti tooth implant corrosion
Open Research DataThe dataset contains micrographs made with a scanning electron microscope (SEM) Hitachi S-3400N of the tooth implant removed after inflammation. The inflammation was induced by the increased corrosion rate of the titanium screw. The reason for the corrosion to occur was the appearance of the concentration cell of different aeration for various areas...
-
Hydrogenation process ofTiO2/BiVO4/PEDOT:PSS observed by XPS method
Open Research DataTitania nanotubes synthesis was based on a two-stage anodization process at water/ethylene glycol (5%/95%) electrolyte containing 0.27 M NH4F and 1 M H3PO4 described previously. Anodization process was performed in two-electrode cell compartment using platinum mesh as a cathode. The distance between electrodes was about 2 cm. The anodization voltage...