Search results for: in situ exsolution
-
Designing high-performance quasi-symmetrical solid oxide cells with a facile chemical modification strategy for Sr2Fe2−xWxO6−δ ferrites electrodes with in situ exsolution of nanoparticles
Publication -
Exsolution of Ni nanoparticles on the surface of cerium and nickel co-doped lanthanum strontium titanate as a new anodic layer for DIR-SOFC. Anti-coking potential and H2S poisoning resistance of the prepared material
PublicationThe aim of this study was to evaluate a new catalytic material for biogas fueled DIR-SOFC. This material was a perovskite-type SrTiO3 doped with La, Ce and Ni of a general formula La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-σ (LSCNT). Additional preparation steps were undertaken to promote a nickel exsolution process. Heat post-treatment of powders in a humidified H2 resulted in an intensive growth of nickel nanoparticles (NPs) while the temperature...
-
SEM images of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me=Co, Fe, Ni) powder materials after reduction at 1000 deg.C in hydrogen
Open Research DataThe dataset presents SEM images of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me=Co, Fe, Ni) powder materials after reduction at 1000 deg.C in hydrogen. The powders were synthesized via the Pechini method. The reduction was performed in order to force the exsolution process of metallic nanoparticles.
-
SEM images of (La0.3Sr0.6Ce0.1)0.9(Me1Me2Ti)O3-δ (Me1,Me2=Co, Fe, Ni) powder materials after reduction at 1000 deg.C in hydrogen
Open Research DataThe dataset presents SEM images of (La0.3Sr0.6Ce0.1)0.9(Me1Me2Ti)O3-δ (Me1,Me2=Co, Fe, Ni) powder materials after reduction at 1000 deg.C in hydrogen. The powders were synthesized via the Pechini method. The reduction was performed to force the exsolution process of bimetallic nanoparticles.
-
The XRD diffraction patterns of (La0.3Sr0.6Ce0.1)0.9FexTi(1-x)O3-δ (x=0.1, 0.2 and 0.3) materials after reduction at 900 deg.C in hydrogen
Open Research DataThe (La0.3Sr0.6Ce0.1)0.9FexTi(1-x)O3-δ (x=0.1, 0.2 and 0.3) materials were synthesized via the Pechini method. First, the reagents in the form of nitrates were weighed and dissolved in DI water. In another beaker, a stoichiometric amount of titanium (IV) butoxide (Ti(OBu)4) was mixed together with reagent-grade ethylene glycol (EG), and citric acid...
-
Kun Zheng dr hab. inż.
People