  • Nonlinear impedance of vanadate glass-ceramics containing BaTiO3

    Dane Badawcze

    The nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...

  • The morphology of vanadate glass-ceramics containing BaTiO3 measured with the use of AFM

    Dane Badawcze

    The structure of vanadate glass-ceramics doped with BaTiO3 was measured by AFM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...

  • The morphology of vanadate glasses containing BaTiO3 measured with the use of AFM

    Dane Badawcze

    The morphology of vanadate glasses doped with BaTiO3 was measured with the use of AFM method. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured...

  • Nonlinear impedance of vanadate glasses containing BaTiO3

    Dane Badawcze

    The nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...

  • The structure of vanadate glass-ceramics containing BaTiO3 measured with X-ray diffraction method

    Dane Badawcze
    open access

    The structure of vanadate glass-ceramics doped with BaTiO3 was measured by XRD. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...

  • The structure of vanadate glass-ceramics containing BaTiO3.

    Dane Badawcze

    The structure of vanadate glass-ceramics doped with BaTiO3 was measured by SEM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...

  • The structure of vanadate glasses containing BaTiO3.

    Dane Badawcze

    The structure of vanadate glasses doped with BaTiO3 was measured by SEM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...

  • The morphology of vanadate glass-ceramics containing BaTiO3

    Dane Badawcze
    open access

    The morphology of vanadate glass-ceramic doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...

  • The morphology of vanadate glasses containing BaTiO3

    Dane Badawcze
    open access

    The morphology of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573 K) brass...

  • Linear impedance of vanadate glass-ceramics containing BaTiO3

    Dane Badawcze

    The linear impedance of vanadate glass-ceramics containing BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...

  • Linear impedance of vanadate glasses containing BaTiO3

    Dane Badawcze

    The linear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...