ISSN:
eISSN:
Publisher:
Disciplines
(Field of Science):
- biomedical engineering (Engineering and Technology)
- chemical engineering (Engineering and Technology)
- civil engineering, geodesy and transport (Engineering and Technology)
- materials engineering (Engineering and Technology)
- mechanical engineering (Engineering and Technology)
- pharmacology and pharmacy (Medical and Health Sciences )
- chemical sciences (Natural sciences)
(Field of Science)
Ministry points: Help
Year | Points | List |
---|---|---|
Year 2024 | 40 | Ministry scored journals list 2024 |
Year | Points | List |
---|---|---|
2024 | 40 | Ministry scored journals list 2024 |
2023 | 70 | Ministry Scored Journals List |
2022 | 40 | Ministry Scored Journals List 2019-2022 |
2021 | 40 | Ministry Scored Journals List 2019-2022 |
2020 | 40 | Ministry Scored Journals List 2019-2022 |
2019 | 40 | Ministry Scored Journals List 2019-2022 |
2018 | 11 | B |
2017 | 11 | B |
2016 | 11 | B |
2015 | 11 | B |
2014 | 9 | B |
2013 | 9 | B |
2012 | 6 | B |
2011 | 6 | B |
2010 | 6 | B |
Model:
Impact Factor:
Publishing policy:
- License
- open in new tab
- Information on publishing policy
- https://content.sciendo.com/view/journals/adms/adms-overview.xml open in new tab
- Information on the conditions of self-archiving
- Included in license
- Is self-archiving allowed by the journal?
- Yes - with restrictions
- Information on research data policy
- n/a
- Months of embargo
- no embargo
- Additional information
-
Must link to journal homepage with DOI.
Self-archiving policy for article versions based on the Sherpa Romeo database.
Papers published in journal
Filters
total: 135
Catalog Journals
-
ADVANCES IN MATERIALS SCIENCE EDITORIAL ON THE JOURNAL'S 20th ANNIVERSARY
PublicationEditorial on the occasion of the 20th anniversary of Advances in Materials Science journal.
-
X-Ray Computer Tomography Study of Degradation of the Zircaloy-2 Tubes Oxidized at High Temperatures
PublicationThe investigations of high-temperature oxidation of zirconium alloys, applied for fuel pellets in nuclear power plants, are usually limited to oxidation kinetics, phase transformations and microstructural characterization. The purpose of this research was to characterize the degradation phenomena occurring within oxide layer and at the interface oxide/metal, on internal and external Zircaloy-2 tube...
-
Influence of Nitriding and Laser Remelting on Properties of Austenitic Stainless Steel Type X10CrNi18-8 and Cavitation Erosion Resistance
PublicationThe paper presents properties of surface layers. Surface layers were obtained by using low temperature glow–discharge nitriding process and laser remelting carried out on austenitic stainless steel type X10CrNi18-8. Investigations were done by using an Ultra Nanoindentation Tester (UNHT) in the Warsaw Institute of Fundamental Technological Research. The influence of the above mentioned...
-
Influence of sulphur on high temperature degradation of steel structures in the refinery industry
PublicationArtykuł stanowi przegląd skutków wpływu związków siarki, znajdujących się w mediach procesowych instalacji rafineryjnych, na elementy konstrukcji ze stali węglowych i stopowych. Wyróżniono dwa aspekty wysokotemperaturowej korozji siarkowej: związany z tworzeniem się zgorzeliny siarczkowej i ubytkami masy oraz dotyczący wewnętrznej degradacji elementu w wyniku zmian mikrostruktury stali. Przedstawiono tzw. zmodyfikowane krzywe McConomy...
-
Low velocity impact damage in glass/polyester composite sandwich panels
PublicationZbadano odporność udarową konstrukcji przekładkowych z laminatu poliestrowo szklanego pod kątem adhezji z rdzeniem (pianki PVC) przy polaczeniu dwoma rodzajami kleju lub łączanymi na ''mokro'' przy pomocy żywicy w trakcie utwardzania laminatu. Do oceny obszaru zniszczeń udarowych zastosowano metodę ultradźwiękową, która umożliwia wykrycie pola delaminacji nakładających się na siebie w poszczególnych warstwach .Obszary zniszczeń...
-
Estimation of cavitation erosion resistance of materials
PublicationW pracy przedstawiono ocenę odporności kawitacyjnej 17 materiałów. Do opisu odporności kawitacyjnej zaproponowano nowy wskaźnik liczbowy uwzględniający długość okresu inkubacji, maksymalną prędkość niszczenia oraz czas po którym wystąpi maksymalna prędkość niszczenia materiału. Zaproponowany wskaźnik porównano ze wskaźnikiem δcav, który reprezentuje całą krzywą erozji kawitacyjnej materiału.
-
Environmental degradation of the Cr-Mo steels in liquid hydrocarbons
PublicationPrzedstawiono podatność stali stopwych 26H2MF i 34HNM do naprężeniowego pękania korozyjnego. Środowiskiem do badań było paliwo ciężkie i zużyty olej mineralny.
-
Numerical modelling of asymetric double-layer Al-Cu plate rolling process
PublicationNiekorzystnym zjawiskiem towarzyszącym procesom walcowania płaskich wyrobów bimetalowych jest krzywizna pasma na wyjściu z kotliny walcowniczej wynikająca z nierównomierności odkształcenia warstw bimetalowej blachy. Możliwość szybkiego i łatwego przeciwdziałania temu zjawisku daje wprowadzenie asymetrii prędkości bądź średnic walców roboczych. W przedstawionym artykule zaprezentowano badania komputerowe procesu walcowania blach...
-
New laser-enhanced surface treatment of Ti bioalloy
PublicationPrzedstawiono wyniki badan mikrostruktury i korozji w roztworze Ringera stopu Ti6Al4V, który był poddawany nadtapianiu laserem CO2 w powietrzu, wodzie i ciekłym azocie. Stwierdzono znaczący wpływ warunków obróbki na mikrostrukturę, mikrotwardość i głębokość zmodyfikowanej warstwy wierzchniej.
-
Hydrogen permeation through welded joints of S690QL steels at cathodic polarisation in sea water in the presence of SRB
PublicationPrezentowane są wyniki badan metodą Devanathana- Stachurskyego przenikania wodoru w wodzie morskiej w obecności bakterii redukujących siarczany i w warunkach sterylnych. Badania wykonano na stali S690QL poddanej symulowanym obróbkom cieplnym prowadzącym do struktur modelujących strefy wpływu ciepła. Stwierdzono dodatni wpływ obecności bakterii na przenikanie wodoru. Różnice między poszczególnymi próbkami były minimalne.
-
The use of nitriding as a prevention method against hydrogen degradation of high-strength steels
PublicationPrzedstawiono badania wpływu warstw azotowanych jarzeniowo na stali 34CrAlNi7-10 na jej podatność na niszczenie wodorowe. Wytworzono warstwy azotowane w atmosferach technologicznych o różnym udziale wodoru. Próbki materiału rodzimego i z warstwami azotowanymi poddano próbie rozciągania z małą prędkością odkształcania w środowisku 0,01 N kwasu siarkowego przy polaryzcaji katodowej. Względny spadek plastyczności i charakter przełomu...
-
Microstructural aspects of corrosion of the SUPERSTON alloy after laser treatment
PublicationW artykule przedstawiono rezultaty obróbki laserowej stopu SUPERSTON w warunkach kriogenicznych i jej wpływ na mikrostrukturę i odporność korozyjną. Badania korozyjne zostały zrealizowane metodą potencjostatyczną w 3% NaCl, odporność korozyjna stopu zmieniała się wraz ze zmianą parametrów nadtapiania laserowego.
-
Corrosion and hydrogen intake for some Cr-Mn steels in liquid hydrocarbons
PublicationStal 34HNM i 26H2MF, poddana różnym obróbkom cieplnym wykazała skłonność do korozji naprężeniowej przy pomiarach ze stałą szybkością rozciągania (10-6s-1) i pomiarach niskocyklowego zmęczenia, wykonanych w paliwie kotłowym. Mechanizm korozji naprężeniowej określono jako kruchość wodorowa, co zostało potwierdzone w pomiarach pochłaniania wodoru z tych środowisk. Jako możliwe źródła wnikania wodoru do stali omówiono procesy korozyjne,...
-
Environmental degradation of titanium biomaterials: mechanisms, effects, testing and evaluation
PublicationPrzedyskutowano możliwe przyczyny oraz mechanizmy degradacji biomateriałów tytanowych, używanych jako długoterminowe implanty stawów. Dokonano przeglądu wpływu impalntów metalicznych w ludzkim ciele. Przedstawiono bieżące procedury badania oraz ich wady. Zaproponowano procedurę oszacowania biomateriałów na implanty.
-
Hydrogen degradation of high strength weldable steels
PublicationW pracy przedstawiono wyniki badań podatności stali spawalnych o wysokiej wytrzymałości na niszczenie wodorowe. Badano dwa gatunki stali S690Q i ich złącza spawane. Ocenę podatności na niszczenie wodorowe wykonano w oparciu o próbę rozciągania z małą prędkością odkształcania w powietrzu i środowisku wody morskiej przy polaryzacji katodowej. Przedstawiono model niszczenia wodorowego badanych stali i ich złączy spawanych.
-
Wpływ utleniania w wysokich temperaturach na struktury napawanych warstw na bazie kobaltu
PublicationPrzedmiotem badań są napawane plazmowo warstwy wykonane ze stopu kobaltu zawierające ok. 29% chromu, ok. 5% wolframu i ok. 2% niklu, nałożone powierzchnie przylgni grzybków zaworów wylotowych silnika dieslowskiego. Powierzchnia podlega zarówno oddziaływaniom temperatury i środowiska, jak i oddziaływaniom mechanicznym. Podczas badań warstwy poddano oddziaływaniu środowiska utleniającego i wysokich temperatur: 750°C- górna w normalnej...
-
The degradation of metal implants
PublicationThe presence of metal implants in the human body causes some dangers, which result from introducing another object into organism. There may occur a biocorrosion, which causes different modifications of implant surface.
-
Analisys of the failure of fixator used in bone surgery
PublicationThe Gamma nail (fixator) made of stainless steel, which has broken in the body, was subjected to examination. The fixator was removed from the patient femur. The fracture occurred in the area of the nail hole after two months' stay in the organism. The research included chemical composition, hardness of the Gamma nail material and the observation and analysis of the type of fracture. The research showed the fatigue failure of the...
-
Cavitation erosion of X5CrNi18-10 austenitic stainless steel alloyed with TiC
PublicationPraca prezentuje zmianę odporności kawitacyjnej stali X5CrNi18-10 po laserowym stopowaniu jej warstwy wierzchniej węglikiem TiC. Laserowe stopowanie przeprowadzono dla 2 wariantów. W pierwszym przypadku stal stopowano do zawartości 1,55 TiC a w drugim do zawartości 3,97% TiC. Uzyskane rezultaty wskazują że przy zawartości 3,97 TiC nastopiło znaczące zwiększenie odporności na plastyczne odkszyałcenie warstwy wierzchniej pod wpływem...
-
Microstructure and corrosion properties of the (Mn-N-O-P) type layers created on aluminium alloys
PublicationPrzedstawiono mikrostrukturę i właściwości korozyjne warstw powierzchniowych typu (Mn-N-O-P) wytworzonych na stopach aluminium. Wykazano, iż warstwy (Mn-N-O-P) podwyższają wielokrotnie odporność korozyjną stopów aluminium i mogą być stosowane jako warstwy ochronne na tych materiałach.
-
Stabilization of the titanium vibration damping wires in the steam turbine blades system
PublicationPrzedstawiono metody stabilizacji drutów tłumiących w systemie łopatkowym turbin parowych. Na podstawie badań eksperymentalnych mikrostruktury i własności mechanicznych wykazano przydatność metody stabilizacji na gorąco drutów tłumiących wykonywanych ze stopu tytanu WT3-1.
-
Underwater welding - a review
PublicationW artykule przedstawiono stan obecny oraz perspektywy rozwoju technik spawania pod wodą. Przeanalizowano najważniejsze problemy spawania w środowisku wodnym. Przedstawiono najważniejsze kierunki badań spawania podwodnego podejmowane w Katedrze Technologii Materiałów Maszynowych i Spawalnictwa Politechniki Gdańskiej
-
Surface cracking of laser melted Ti-6Al-4V alloy
PublicationOpisano charakterystyczne cechy pękania powierzchniowego obserwowanego po nadtapianiu laserem CO2 i Nd:YAG stopu Ti-6Al-4V. Obserwowano pęknięcia niezależnie od sposobu nadtapiania, penetrujące głęboko strefę przetopioną i w niewielkim stopniu zależne od sposobu nadtapiania. Przypisano obserwowane zjawisko przemianie martenzytycznej i (lub) naprężeniom cieplnym powstającym podczas gwałtownego chłodzenia.
-
Effects of the time and temperature on the oxide scale formed on the cobalt alloys
PublicationWarstwy wykonane za pomocą techniki PTA ze stopu kobaltu poddano utlenianiu w różnych temperaturach i w różnym czasie. Mikrostruktury otrzymane po utlenianiu wskazują na proces degradacji materiału. Proces ten prowadził do degradacji obszarów międzydendrytycznych napoiny. Skład chemiczny powstającej zgorzeliny byłzależny od temperatury utleniania, składu chemicznego stopu, ze szczegfólnym uwzględnieniem obecności małych ilości...
-
FEM approach to estimate the behaviour of biocomposite metal-surface coating system
PublicationA three dimensional (3D) model of biocomposite metal-surface coating system, which is influenced byknown external forces, is proposed. This model consists of the metallic substrate (Ti6Al4V) and thehydroxyapatite (HA) coating. Using FEM (finite element method), strain-stress maps of model weregenerated for investigating relations between the extreme stress of HA coating and the magnitude ofexternal force and the thickness of the...
-
Coatings in arthroplasty [online]
PublicationThe modern coatings used in arthroplasty for long term implants are reviewed. The phosphate coatingsare the most popular technique to improve the bone-implant interfacial strength and promote theosseointegration. The plasma spraying, electrophoretic precipitation, powder metallurgy, ion beamsputtering, high velocity oxy-fuel (HVOF) combustion spraying, sol-gel technique, biomimeticdeposition are mostly used to obtain the phosphate,...
-
Allergy to implant components: chromium, nickiel, cobalt and titanium
PublicationImplant jest kompozycja roznych pierwiastkow: niklu, chromu, kobaltu, tytanu, molibdenu i wanadu. Pierwiastki te moga doprowadzic do alergii, egzemy i obluzowania implantu.
-
Effect of chemical composition and microstructure on mechanical properties of BA1055 bronze sand castings.
PublicationW pracy wykazano, że nawet małe zmiany w składzie chemicznym brązu aluminiowego BA1055 mają istotny wpływ na strukturę i właściwości mechaniczne odlewów. Określono wpływ wydzieleń międzymetalicznej fazy κ na właściwości odlewów z brązu BA1055 stosowanego na pędniki okrętowe.
-
Optoelectronic system for investigation of cvd diamond/DLC layers growth
PublicationDevelopment of the optoelectronic system for non-invasive monitoring of diamond/DLC (Diamond-Like-Carbon) thin films growth during μPA ECR CVD (Microwave Plasma Assisted Electron Cyclotron Resonance Chemical Vapour Deposition) process is described. The system uses multi-point Optical Emission Spectroscopy (OES) and long-working-distance Raman spectroscopy. Dissociation of H2 molecules, excitation and ionization of hydrogen atoms...
-
Environmental degradation of titanium alloy in artificial saliva
PublicationThe titanium and its alloys are potentially prone to hydrogen embrittlement, including those proposed for dental implants. The research has been aimed to assess a susceptibility to environment-enhanced degradation of the Ti-13Zr-13Nb alloy in artificial saliva with or without hydrofluoric acid, subject or not to cathodic polarisation. The results have shown that even if artificial saliva is safe environment, both cathodic polarization...
-
Novel Polyurethanes as Antifouling Paint Matrices
PublicationThe new poly(ester-ether urethane)s (PEEUR) were prepared in two stage synthesis from formerly obtained oligo(alkylene ester-ether)diols (OAEE) and 4,4‘-diphenylmethane diisocyanate (MDI). PEEUR samples were subjected to crosslinking with styrene in the presence of radical polymerization initiators: methyl ethyl ketone peroxide (MEKPO) or cobalt 2-ethyl cyclohexanoate (EtHCo). Crosslinked PEEUR were characterized by their physicochemical...
-
Modeling by finite element methods of impact of erosion on frequency of normal modes of L-0 blade
PublicationAfter some time of exploitation steam turbine rotors blades in energetic industry they are being eroded and also their frequency of normal modes is changed. Those changes can cause to unwanted shift of blades normal mode frequencies. It is necessary to find quick method of rating changes of frequency in connection of mass loss due erosion. The evaluation of this dependence was made by finite element modeling method using HyperWorks...
-
Allergic Reactions as a Defense of the Organism to the Influence of Implants Components Made of Stainless Steel
PublicationDue to the increasing number of cases of hypersensitivity caused by direct contact with metals, as well as the increasing demand for implants in humans all ages numerous studies on the effects of the impact of implant components are being carried out. The paper presents the phenomenon of etiology of allergy in general terms and in relation to the biomaterials used in medicine. There have been characterized in terms of impact on...
-
Corrosion resistance examinations of Ti6Al4V alloy with the use of potentiodynamic method in Ringer`s and artificial saliva solutions
PublicationThe research results of corrosion resistance of the Ti6Al4V alloy in the simulated body fluids (SBF) are presented. The polished specimens have shown better corrosion resistance than grinded surfaces in both liquids. The artificial saliva has revealed more aggressive test solution than Ringer`s solution. The pitting tendency has been observed in Ringer`s solution for grinded specimens.
-
Properties of surface layers of titanium alloy Ti6Al4V after laser melting processes
PublicationThe article presents the investigation results of titanium alloy Ti6Al4V surface layer after laser melting process. The process of laser melting was performed using Nd-YAG laser. The evaluation of structure of the alloy as well as hardness and chemical composition was performed. It was shown that laser melting changes the structure and properties of titanium alloy Ti6Al4V and process parameters as scanning speed affects the thickness...
-
Failure analysis of the exhaust valve face in diesel marine engine
PublicationThe exhaust valve from marine diesel engine which was damaged after 2000 hours of service was investigated. In order to prolong the service time the valve face was cladded with cobalt base alloy using laser technique. After failure microstructural and chemical analyses reviled that cladding process was conducted improperly. The chemical composition of the clad layer was far from the designed one and what more completely inhomogeneous....
-
Fracture Energy of Bonded Joints with 2D Elastic Adhesive Layer
PublicationWhen bonded joint is subjected to mode I fracture loading, the adhesive joints analytical solutions treats the adhesive layer, usually, as not existing or 1D Hooke elastic layer. In the case of 1D elastic layer, represented as Hookes spring element, is acting, only, in direction contrary to the applied load. Basing on the information yielded from sensitive laser profilometry technique, where deflections of bonded part of the joint...
-
Assessment of fitness for service of Cr-Mo steel tubes in catalytic reforming charge heaters
PublicationIn this paper characteristic features of metal dusting corrosion in high temperature gas mixtures of high carbon activity in catalytic reforming units, including Continuous Catalyst Regeneration (CCR) platformer are presented. Examples of 2.25Cr-1Mo and 9Cr-1Mo steel tubes at advanced stages of metal dusting process after long-term service in charge heaters are used to prove that destructive examinations are necessary to provide...
-
Reactions on the surface of the implant under the influence of biofilm
PublicationThe contact of a biomaterial with the biological environment in in vitro and in vivo tests leads to the production of a particular ecosystem in which the active roles perform both, the material surface and the extracellular matrix protein forming a biofilm. Proteins affect cell and bacteria adhesion processes, biological activity of cells and activation of inflammatory response.The knowledge of the reaction mechanisms active on...
-
Preparation of silver nanoparticles in reverse micelles and antibacterial activity of silver modified-paints
PublicationW publikacji została opisana metoda otrzymywania nanocząstek srebra oraz farb modyfikowanych srebrem i ich wpływ na zahamowanie rozwoju wybranych bakterii i grzybów. Podjęto również próbę porównania wpływu rodzaju prekursora srebra oraz substancji powierzchniowo czynnej na stabilność otrzymanych nanocząstek srebra. Przygotowane mikroemulsje zawierały od 500 do 2000 ppm srebra
-
Allergic reactions as a defense of the organism to the influence of implants components made of stainless steel
PublicationDue to the increasing number of cases of hypersensitivity caused by direct contact with metals, as well as the increasing demand for implants in humans all ages numerous studies on the effects of the impact of implant components are being carried out. The paper presents the phenomenon of etiology of allergy in general terms and in relation to the biomaterials used in medicine. There have been characterized in terms of impact on...
-
Two tests for adhesive bonding long term characterization: principles and applications
PublicationThis article describes recent refinement of the traditional wedge test technique used to characterize durability of the adhesive joints. We propose two types of measuring protocols to monitor precisely and continuously the propagation of an "effective" crack during long term mode I fracture mechanic test. First method is directly derived from the traditional wedge test technique and consist in monitoring the surface strain of adherent...
-
Porous biomaterial for orthopaedic implants based on titanium alloy
PublicationTytan i jego stopy są szeroko stosowane jako biomateriały dla zastosowań ortopedycznych. Badania związane z ich najlepszą odpornością na korozję i ścieranie, biozgodnością i bioaktywnością są stale prowadzone. Obecne badania koncentrują się również na projektowaniu i produkcji materiałów porowatych w oparciu o stopy np. Ti-13Nb-13Zr, które mogą być stosowane do wytwarzania implantów. Jedną z najbardziej efektywnych metod wytwarzania...
-
A Multi Rig Screening Test for Thin Ceramic Coatings in Bio - Tribological Applications
PublicationA method is presented for the comparative testing of wear resistance of ceramic coatings made from materials potentially feasible in tribo - medical applications, mainly orthopaedic implants made from ceramics coated metals for low cost, long life and low wear particle emission into the body. The method was devised as the main tool for use in research and is comprised of flat on flat and ball on flat surface (sliding) tests. Seven...
-
Nanotechnologies in Development of Structural Materials and Biomaterials
PublicationThe nanometric materials and technologies resulted in nanostructures are reviewed. The examples of nanomaterials are shown. The typical nanotechnologies, including plastic deformation, mechanical attrition, controlled detonation, hot plasma jet synthesis, laser vaporisation, CVD and PVD, mechanical milling, annealing, ultrasonic irradiation, nanolithography, electrocrystallisation, electrospinning, sol-gel method, cryogenic laser-enhanced...
-
Influence of pore formers on electrical properties of CaTi0.9Fe0.1O3-δ perovskite-type ceramics
PublicationPorous CaTi0.9Fe0.1O3-δ (CTF) perovskites were synthesized by the standard solid state method at different sintering temperatures with carbon black (CB), corn starch (CS) and potato starch (PS) as pore-forming agents. The ceramic samples of porosity between 9% and 42% with 5 - 40 μm pore sizes, were obtained by a 6 h sintering at either 1130º C or 1200º C of precursor powder prepared at 1470º C. X-ray diffraction analysis proved...
-
Resistance to cold cracking of steel joints of P460NL1 steel
PublicationPrzedstawiono wyniki badań odporności na zimne pękanie złączy spawanych ze stali przeznaczonej do pracy pod ciśnieniem. Badano równoczesny wpływ zawartości wodoru dyfundującego i energii liniowej na naprężenie krytyczne w próbie implant dla złączy spawanych elektrodami otulonymi i drutem proszkowym w osłonie gazów ochronnych. Stwierdzono wpływ energii liniowej jak i zawartości wodoru dyfundującego na odporność na zimne pękanie...
-
Hardness measurements for assessment of cavitation intensity
PublicationArtykuł opisuje możliwość zastosowania pomiarów teardości erodowanego materiału do oceny natężenia zjawiska kawitacji. Proponowana metoda zakłada, że cała energia implodujących pęcherzyków kawitacyjnych zamieniana jest na przyrost twardości warstwy wierzchniej materiału
-
Influence of H2S on degradation of 9Cr-1Mo steel in advanced stage of metal dusting process
PublicationPrzedstawiono wyniki badań stali 9Cr-1Mo w zaawansowanym stadium procesu pylenia metalu po 10 latach eksploatacji w piecu rafineryjnej instalacji platformingu CCR, przeprowadzonych w celu podjęcia decyzji o dozowaniu związków siarki do wsadu instalacji. Na podstawie długotrwałej ekspozycji próbek stali w 600C w mieszaninie wodoru i siarkowodoru wykazano, że siarka może być powodem procesów wpływających niekorzystnie na stan materiału...
-
Corrosion resistance of dissimilar austenite and duplex steels welded joints
PublicationW artykule przedstawiono wpływ warunków spawania, a zwłaszcza energii liniowej, na odporność korozyjną złączy różnoimiennych stali austenitycznej 316L i typu duplex 2203. Przedstawiono wyniki testów korozyjnych:korozji wżerowej wg ASTM G48 oraz korozji naprężeniowej badanej w próbach odkształcania z małą pędkością w środowisku roztworu chlorku magnezowego.