Influence of pitting corrosion on fatigue and corrosion fatigue of ship structures. Part I: pitting corrosion of ship structures.

Abstract

The paper is a literature survey focused on pitting corrosion and its influence on fatigue of ship and offshore steels. Mechanisms of short- and long-term pitting corrosion in marine environment have been described including pit nucleation and growth phases. Some models of pit growth versus time of exposure have been presented. Some factors which influence the pit growth have been discussed briefly.

Cite as

Full text

download paper
downloaded 62 times
Publication version
Accepted or Published Version
License
Creative Commons: CC-BY-NC-ND open in new tab

Keywords

Details

Category:
Articles
Type:
artykuł w czasopiśmie wyróżnionym w JCR
Published in:
Polish Maritime Research no. 21, pages 62 - 69,
ISSN: 1233-2585
Language:
English
Publication year:
2014
Bibliographic description:
Jakubowski M.: Influence of pitting corrosion on fatigue and corrosion fatigue of ship structures. Part I: pitting corrosion of ship structures.// Polish Maritime Research. -Vol. 21, iss. 1 (2014), s.62-69
Verified by:
Gdańsk University of Technology

seen 139 times

Recommended for you

Meta Tags