Application of wet powder spraying for anode supported solid oxide fuel cell with a perowskite SrTi0.98Nb0.02O3-d anode
PublicationAnode-supported solid oxide fuel cell with SrTi0.98Nb0.02O3–d anode, yttria-stabilized zirconia electrolyte and La(Ni0.6Fe0.4) O3d cathode has been successfully fabricated and evaluated. Process of anode support fabrication has been presented. Wet powder spraying and high temperature sintering method have been studied and applied to deposit the thin electrolyte layer.In order to improve catalytic properties of the anode, it has...
-
Effects of Heat and Momentum Gain Differentiation during Gas Detonation Spraying of FeAl Powder Particles into the Water
Publication -
The XRD diffraction patterns of La0.3Sr1.7Fe1.5Mo0.5O6 powder calcined at 1200oC in air
Open Research DataThe dataset includes XRD patterns of La0.3Sr1.7Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder calcined at 1100oC in air
Open Research DataThe dataset includes XRD patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.5Mo0.5O6 powder calcined at 1100oC in air
Open Research DataThe dataset includes XRD patterns of Sr1.9Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder calcined at 1200oC in air
Open Research DataThe dataset includes XRD patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.5Mo0.5O6 powder calcined at 1200oC in air
Open Research DataThe dataset includes XRD patterns of Sr1.9Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XRD diffraction patterns of La0.3Sr2Al0.1FeMoO6 powder calcined at 1200oC in air
Open Research DataThe dataset includes XRD patterns of La0.3Sr2Al0.1FeMoO6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XRD diffraction patterns of Sr2Al0.1Fe1.4Mo0.5O6 powder calcined at 1100oC in air
Open Research DataThe dataset includes XRD patterns of Sr2Al0.1Fe1.4Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of La0.3Sr1.7Al0.1Fe1.5Mo0.5O6 powder calcined at 1100oC in air
Open Research DataThe dataset includes XRD patterns of La0.3Sr1.7Al0.1Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.