Fourier transform infrared spectroscopy (FTIR) of pre- PXBS (0 h) and PXBS during the crosslinking process (24 h–288 h)
Opis
The goal of this research was developing biodegradable and biocompatibile xylitol-based copolymers with improved mechanical properties, and investigating the change in their thermal and chemical properties with
progress of the cross-linking process. Using a raw material of natural origin such as xylitol, a prepolymer was
obtained by esterification and polycondensation. Then, at subsequent stages of the crosslinking process in a
vacuum dryer, samples of materials were taken to determine the progress of the process using Fourier transform
infrared spectroscopy. The method of differential scanning calorimetry also defined changes in the ranges of
phase changes occurring at each stage of the crosslinking process. After the crosslinking process, ester materials
based on sebacic and succinic acid were characterized in terms of mechanical and surface properties.
Plik z danymi badawczymi
hexmd5(md5(part1)+md5(part2)+...)-{parts_count}
gdzie pojedyncza część pliku jest wielkości 512 MBPrzykładowy skrypt do wyliczenia:
https://github.com/antespi/s3md5
Informacje szczegółowe o pliku
- Licencja:
-
otwiera się w nowej karcieCC BYUznanie autorstwa
- Embargo na plik:
- 2024-05-15
Informacje szczegółowe
- Rok publikacji:
- 2023
- Data zatwierdzenia:
- 2023-12-14
- Data wytworzenia:
- 2019
- Język danych badawczych:
- angielski
- Dyscypliny:
-
- inżynieria materiałowa (Dziedzina nauk inżynieryjno-technicznych)
- DOI:
- Identyfikator DOI 10.34808/a8h3-rp16 otwiera się w nowej karcie
- Weryfikacja:
- Zachodniopomorski Uniwersytet Technologiczny w Szczecinie
Słowa kluczowe
Powiązane zasoby
Cytuj jako
Autorzy
Wersja ten dokument posiada różne wersje
-
Aktualna wersjawersja 1.0Data publikacji wersji 2023-12-14
wyświetlono 130 razy