Filtry
wszystkich: 9
Wyniki wyszukiwania dla: ALLOY 617
-
Dissimilar autogenous TIG joint of Alloy 617 and AISI 304H steel for AUSC application
PublikacjaTo reduce costs and improve high-temperature performance in Advanced Ultra Super Critical (AUSC) boilers, it is necessary to weld austenitic steel to Inconel alloy. In this study, the autogenous tungsten inert gas (TIG) welding process was used to join Alloy 617 and an austenitic AISI 304H steel plate of thickness 5 mm. Microstructural analysis showed that the microstructure formation was uneven along the weldments, with columnar...
-
High-Temperature Tensile Behaviour of GTAW Joints of P92 Steel and Alloy 617 for Two Different Fillers
PublikacjaThis study explores the high-temperature (HT) tensile rupture characteristics of a dissimilar gas-tungsten-arc-welded (GTAW) joint between P92 steel and Alloy 617, fabricated using ER62SB9 and ERNiCrCoMo-1 fillers. The high-temperature tensile tests were performed at elevated temperatures of 550 ◦C and 650 ◦C. An optical microscope (OM) and a field emission scanning electron microscope (FESEM) were utilized to characterize the...
-
Studying the Effect of Working Conditions on WEDM Machining Performance of Super Alloy Inconel 617
PublikacjaWire electrical discharge machining (WEDM) has been for many years a precise and efficient non-conventional manufacturing solution in various industrial applications, mostly involving the use of hard-to machine materials like, among other, the Inconel super alloys. The focus of the present study is on exploring the effect of selected control parameters, including pulse duration, pulse-off time and the dielectric flow pressure on...
-
Role of buttering layer composition on microstructural heterogeneity and mechanical properties of Alloy 617 and P92 steel dissimilar welded joints for future Indian AUSC program
PublikacjaRestrictive operating conditions (even exceeding 700 °C) of materials in advanced ultra super critical (AUSC) power plants and the need to minimize manufacturing and maintenance costs require the production of dissimilar metal welded joints (DMW). Significant differences in the physical and chemical properties of welded materials lead to phenomena that reduce the weldability of the metals used and force the search for solutions...
-
Study on Microstructure-Property Relationship of Inconel 617 Alloy/304L SS Steel Dissimilar Welds Joint
PublikacjaWelding of Inconel 617 (IN617) alloy and austenitic 304L SS steel has been attempted using the autogenous Laser Beam Welding (LBW) process. Characterization of dissimilar weldments was performed on either side of the fusion boundaries. The metallographic results showed that the inhomogeneous microstructure formation for weld metal contained columnar and cellular dendrites near the interface, whilst the columnar, cellular and equiaxed...
-
Metallurgical characterization and high-temperature tensile failure of Inconel 617 alloy welded by GTAW and SMAW—a comparative study
PublikacjaTwo types of the weld joint of Inconel 617 alloy were produced using gas tungsten arc welding (GTAW) and shielded metal arc welding (SMAW) processes with ERNiCrCoMo-1 filler metal and ENiCrCoMo-1 electrode, respectively. The weld metal showed the segregation of the principle alloying elements like Mo and Cr along the inter-dendritic spaces, triggering the formation of secondary phases. The microstructure characterization of the...
-
P92 steel and inconel 617 alloy welds joint produced using ERNiCr-3 filler with GTAW process: Solidification mechanism, microstructure, mechanical properties and residual stresses
PublikacjaThe objective of the current study was to analyse the microstructure, mechanical characteristics, and residual stresses of a dissimilar welded joint (DWJ) made of P92 steel and the Inconel alloy 617 (IN617) using the gas tungsten arc welding (GTAW) method. The ERNiCr-3 filler was selected to produce the conventional V groove (VG) and narrow V groove (NVG) butt joint. The filler deficient zones in the weldments, such as the filler...
-
Microstructure degradation and creep failure study of the dissimilar metal welded joint of heat-resistant steel and Inconel 617 alloy tested at 650 °C and applied stress range of 100–150 MPa
PublikacjaThe advanced ultra-supercritical (A-USC) power plant system is anticipated to become India's next-generation base-load power station. To adopt AUSC technology, dissimilar welded joints (DWJs) between heat-resistant steels and the nickel-based alloys, using the nickel-based fillers, will need to be implemented. However, failure of dissimilar welded joints from P92 steel base metal or the heat affected zone (HAZ) has been commonly...
-
Selection of Electrode Material for Inconel 617/P92 Steel SMAW Dissimilar Welds
PublikacjaThe present work aimed to investigate the microstructure and mechanical properties of the dissimilar shielded metal arc welded (SMAW) joint of Alloy 617 and P92 steel for advanced ultrasupercritical boilers. The SMAW joint was produced using three different types of electrodes, namely, ENiCrFe-3, ENiCrMo-3, and ENiCrCoMo-1. During microstructural observation of the welded joints, no possible cracking was detected in the weldments....