ISSN:
eISSN:
Publisher:
Disciplines
(Field of Science):
- biomedical engineering (Engineering and Technology)
- chemical engineering (Engineering and Technology)
- civil engineering, geodesy and transport (Engineering and Technology)
- materials engineering (Engineering and Technology)
- mechanical engineering (Engineering and Technology)
- pharmacology and pharmacy (Medical and Health Sciences )
- chemical sciences (Natural sciences)
(Field of Science)
Ministry points: Help
Year | Points | List |
---|---|---|
Year 2024 | 40 | Ministry scored journals list 2024 |
Year | Points | List |
---|---|---|
2024 | 40 | Ministry scored journals list 2024 |
2023 | 70 | Ministry Scored Journals List |
2022 | 40 | Ministry Scored Journals List 2019-2022 |
2021 | 40 | Ministry Scored Journals List 2019-2022 |
2020 | 40 | Ministry Scored Journals List 2019-2022 |
2019 | 40 | Ministry Scored Journals List 2019-2022 |
2018 | 11 | B |
2017 | 11 | B |
2016 | 11 | B |
2015 | 11 | B |
2014 | 9 | B |
2013 | 9 | B |
2012 | 6 | B |
2011 | 6 | B |
2010 | 6 | B |
Model:
Impact Factor:
Publishing policy:
- License
- open in new tab
- Information on publishing policy
- https://content.sciendo.com/view/journals/adms/adms-overview.xml open in new tab
- Information on the conditions of self-archiving
- Included in license
- Is self-archiving allowed by the journal?
- Yes - with restrictions
- Information on research data policy
- n/a
- Months of embargo
- no embargo
- Additional information
-
Must link to journal homepage with DOI.
Self-archiving policy for article versions based on the Sherpa Romeo database.
Papers published in journal
Filters
total: 135
Catalog Journals
-
Environmental failure of dental biomaterials
PublicationW pracy przedstawiono problematykę związaną z zagadnieniem trwałości biomateriałów stomatologicznych. Scharakteryzowano kryteria doboru materiałów i na przykładzie koron stomatologicznych pokazano wyniki oceny prawidłowości doboru w oparciu o metodę elementów skończonych. Przedstawiono wyniki weryfikacji doświadczalnej i wskazano na możliwości wykorzystania tej metody do konstruowania odpornych na zniszczenie koron metalowo-ceramicznych.
-
Influence of the heat treatment on corrosion characteristics of the Superston alloy
PublicationW artykule przedstawiono wpływ hartowania i odpuszczania na twardość i właściwości korozyjne stopu Superston, stosowanego na śruby okrętowe. Stwierdzono, iż hartowanie z temperatury 900 st.C i odpuszczanie w temperaturze 550 st.C znacząco podwyższa odporność na korozję stopu Superston w 3% roztworze NaCl w porownaniu ze stanem odlanym.
-
Hardness measurements for assessment of cavitation intensity
PublicationArtykuł opisuje możliwość zastosowania pomiarów teardości erodowanego materiału do oceny natężenia zjawiska kawitacji. Proponowana metoda zakłada, że cała energia implodujących pęcherzyków kawitacyjnych zamieniana jest na przyrost twardości warstwy wierzchniej materiału
-
Influence of H2S on degradation of 9Cr-1Mo steel in advanced stage of metal dusting process
PublicationPrzedstawiono wyniki badań stali 9Cr-1Mo w zaawansowanym stadium procesu pylenia metalu po 10 latach eksploatacji w piecu rafineryjnej instalacji platformingu CCR, przeprowadzonych w celu podjęcia decyzji o dozowaniu związków siarki do wsadu instalacji. Na podstawie długotrwałej ekspozycji próbek stali w 600C w mieszaninie wodoru i siarkowodoru wykazano, że siarka może być powodem procesów wpływających niekorzystnie na stan materiału...
-
Ocena wpływu parametrów nadtapiania laserowego w warunkach kriogenicznych na strukturę warstwy wierzchniej na stopie Ti-6Al-4V
PublicationW pracy zostały przedstawione efekty przetapiania laserowego w warunkach kriogenicznych stopu tytanu Ti-6Al-4V. W celu określenia wpływu obróbki laserowej wykonano analizę mikrostruktury (SEM), składu fazowego (XRD), oraz pomiary mikrotwardości uzyskanych warstw. Stwierdzono, że zmiany podstawowych parametrów przetapiania laserowego - mocy wiązki lasera i prędkości skanowania istotnie wpływają na grubość i mikrostrukturę otrzymanych...
-
Surface cracking of laser melted Ti-6Al-4V alloy
PublicationOpisano charakterystyczne cechy pękania powierzchniowego obserwowanego po nadtapianiu laserem CO2 i Nd:YAG stopu Ti-6Al-4V. Obserwowano pęknięcia niezależnie od sposobu nadtapiania, penetrujące głęboko strefę przetopioną i w niewielkim stopniu zależne od sposobu nadtapiania. Przypisano obserwowane zjawisko przemianie martenzytycznej i (lub) naprężeniom cieplnym powstającym podczas gwałtownego chłodzenia.
-
Effects of the time and temperature on the oxide scale formed on the cobalt alloys
PublicationWarstwy wykonane za pomocą techniki PTA ze stopu kobaltu poddano utlenianiu w różnych temperaturach i w różnym czasie. Mikrostruktury otrzymane po utlenianiu wskazują na proces degradacji materiału. Proces ten prowadził do degradacji obszarów międzydendrytycznych napoiny. Skład chemiczny powstającej zgorzeliny byłzależny od temperatury utleniania, składu chemicznego stopu, ze szczegfólnym uwzględnieniem obecności małych ilości...
-
Underwater welding - a review
PublicationW artykule przedstawiono stan obecny oraz perspektywy rozwoju technik spawania pod wodą. Przeanalizowano najważniejsze problemy spawania w środowisku wodnym. Przedstawiono najważniejsze kierunki badań spawania podwodnego podejmowane w Katedrze Technologii Materiałów Maszynowych i Spawalnictwa Politechniki Gdańskiej
-
Coatings in arthroplasty [online]
PublicationThe modern coatings used in arthroplasty for long term implants are reviewed. The phosphate coatingsare the most popular technique to improve the bone-implant interfacial strength and promote theosseointegration. The plasma spraying, electrophoretic precipitation, powder metallurgy, ion beamsputtering, high velocity oxy-fuel (HVOF) combustion spraying, sol-gel technique, biomimeticdeposition are mostly used to obtain the phosphate,...
-
FEM approach to estimate the behaviour of biocomposite metal-surface coating system
PublicationA three dimensional (3D) model of biocomposite metal-surface coating system, which is influenced byknown external forces, is proposed. This model consists of the metallic substrate (Ti6Al4V) and thehydroxyapatite (HA) coating. Using FEM (finite element method), strain-stress maps of model weregenerated for investigating relations between the extreme stress of HA coating and the magnitude ofexternal force and the thickness of the...
-
Allergy to implant components: chromium, nickiel, cobalt and titanium
PublicationImplant jest kompozycja roznych pierwiastkow: niklu, chromu, kobaltu, tytanu, molibdenu i wanadu. Pierwiastki te moga doprowadzic do alergii, egzemy i obluzowania implantu.
-
Effect of chemical composition and microstructure on mechanical properties of BA1055 bronze sand castings.
PublicationW pracy wykazano, że nawet małe zmiany w składzie chemicznym brązu aluminiowego BA1055 mają istotny wpływ na strukturę i właściwości mechaniczne odlewów. Określono wpływ wydzieleń międzymetalicznej fazy κ na właściwości odlewów z brązu BA1055 stosowanego na pędniki okrętowe.
-
Optoelectronic system for investigation of cvd diamond/DLC layers growth
PublicationDevelopment of the optoelectronic system for non-invasive monitoring of diamond/DLC (Diamond-Like-Carbon) thin films growth during μPA ECR CVD (Microwave Plasma Assisted Electron Cyclotron Resonance Chemical Vapour Deposition) process is described. The system uses multi-point Optical Emission Spectroscopy (OES) and long-working-distance Raman spectroscopy. Dissociation of H2 molecules, excitation and ionization of hydrogen atoms...
-
Low velocity impact damage in glass/polyester composite sandwich panels
PublicationZbadano odporność udarową konstrukcji przekładkowych z laminatu poliestrowo szklanego pod kątem adhezji z rdzeniem (pianki PVC) przy polaczeniu dwoma rodzajami kleju lub łączanymi na ''mokro'' przy pomocy żywicy w trakcie utwardzania laminatu. Do oceny obszaru zniszczeń udarowych zastosowano metodę ultradźwiękową, która umożliwia wykrycie pola delaminacji nakładających się na siebie w poszczególnych warstwach .Obszary zniszczeń...
-
Influence of sulphur on high temperature degradation of steel structures in the refinery industry
PublicationArtykuł stanowi przegląd skutków wpływu związków siarki, znajdujących się w mediach procesowych instalacji rafineryjnych, na elementy konstrukcji ze stali węglowych i stopowych. Wyróżniono dwa aspekty wysokotemperaturowej korozji siarkowej: związany z tworzeniem się zgorzeliny siarczkowej i ubytkami masy oraz dotyczący wewnętrznej degradacji elementu w wyniku zmian mikrostruktury stali. Przedstawiono tzw. zmodyfikowane krzywe McConomy...
-
Estimation of cavitation erosion resistance of materials
PublicationW pracy przedstawiono ocenę odporności kawitacyjnej 17 materiałów. Do opisu odporności kawitacyjnej zaproponowano nowy wskaźnik liczbowy uwzględniający długość okresu inkubacji, maksymalną prędkość niszczenia oraz czas po którym wystąpi maksymalna prędkość niszczenia materiału. Zaproponowany wskaźnik porównano ze wskaźnikiem δcav, który reprezentuje całą krzywą erozji kawitacyjnej materiału.
-
Influence of retrogression and reaging (RRA) heat treatment on microstructure, mechanical and chemical behaviour of an Al-Zn-Mg alloy
PublicationBadano metodą stałego wolnego rozciągania w wodzie morskiej wpływ czasu i temperatury nawrotu oraz powtórnego starzenia na czas do zniszczenia, energię zniszczenia, przewężenie i odkształcenie. Stwierdzono ogólnie niewielki wpływ, przy czym wzrostowi odporności na korozję naprężeniową towarzyszył spadek właściwości mechanicznych. Obserwowane zmiany właściwości przypisano zmianom struktury dyslokacyjnej i mikrostruktury.
-
Relationship between cavitation resistance of laser produced alloys and their ability to work hardening
PublicationBadano odporność kawitacyjną laserowo wytworzonych stopów na stalach konstrukcyjnych i ich związek ze zdolnością do umacniania się pod wpływem działania obciążeń kawitacyjnych. Wykazano, że mikrotwardość powierzchni wykazuje monotoniczną zależność z odpornością kawitacyjną i zdolnością do umacniania.
-
Dependence of cavitation performance of superficial iron alloys on the sub-strate
PublicationWykazano zależność odporności kawitacyjnej laserowo wytworzonych i elektrodąotuloną napawanych powłok od rodzaju podłoża. Napoiny wykonywano na stali 45, 2H13, 0H18N9 i na żelazie Armco.
-
Hydrogen-enhanced stress corrosion cracking in low alloy steels in seawater
PublicationBadano podatność stali niskostopowych w wodzie morskiej w warunkach polaryzacji katodowej. Stwierdzono spadek czasu do zniszczenia, energii zniszczenia i przewężenia ze wzrostem potencjału katodowego. Wykazano znaczącą korelację między stopniem degradacji wodorowej a stężeniem wodoru dyfuzyjnego.
seen 2196 times