SEM image and line EDS of SrTi0.50Fe0.50O3-d porous electrode sintered at 800 °C
Open Research DataThis dataset contains image of the SrTi0.50Fe0.50O3-d porous electrode sintered at 800 °C with line EDS analysis results. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage of 20 kV in a high vacuum mode. The chemical compositions of the investigated powder...
-
SEM micrographs of V2O5 nanocrystals as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 nanocrystals as cathode materials before and after the galvanostatic charge/discharge curves.
-
SEM micrographs of V2O5 nanorods as cathode material in Li-ion batteries
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 nanorods as cathode materials before and after the galvanostatic charge/discharge curves.
-
SEM micrographs of morphology evolution of V2O5 nanostructures
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of morphology evolution of vanadium pentaoxide nanostructures obtained by the sol-gel, depending on annealing temperature under synthetic air. The results show that the morphology dependent on the annealing temperature.
-
SEM micrographs of morphology evolution of V2O3 nanostructures
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O3 nanostructures obtained by the sol-gel with different reaction conditions. The xerogel powder was annealing under a reducing atmosphere (94% Ar, 6% H2) in the temperature range 350-700C. The results show that the morphology dependent on the annealing temperature.
-
SEM micrographs of the V2O5 coatings after thermal treatment under reducing atmosphere
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 coatings on the silicon substrate after thermal treatment under a reducing atmosphere. Thin films were annealed at 600C and 700C for 10 under a reducing atmosphere (94% Ar, 6% H2).
-
SEM micrographs of the V2O5 nanorods after thermal treatment under reducing atmosphere
Open Research DataThe DataSet contains the SEM micrographs of V2O5 nanorods after thermal treatment under a reducing atmosphere. Samples were annealed at 450C for 2, 20, and 40h under a reducing atmosphere (94% Ar, 6% H2).
-
SEM micrographs of VO2 and V6O13 nanostructures
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V6O13 thin films deposited on a silicon substrate. The as-prepared thin films were annealing under a reducing atmosphere (94% Ar, 6% H2) at 600 and 700C for 10h.
-
SEM micrographs of morphology evolution of V2O5 thin films on silicon substrate
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on a silicon substrate. The as-prepared thin films were annealing under an oxidizing atmosphere in the temperature range 250-600C. The results show that the morphology of the films dependent on the annealing temperature.
-
SEM micrographs of ammonium vanadate nanocrystals
Open Research DataThe DataSet contains the electron microscopy (SEM) micrographs of ammonium vanadate nanobelts obtained by the hydrothermal method with different conditions. The results show that the morphology of samples dependent on reaction conditions.
-
SEM micrographs of NH4VO3 crystals - molar concetration factor after annealing
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of NH4VO3 nano_crystals obtained by the LPE-IonEx method with different morphology after annealing at 400C under argon atmosphere (with a heating rate of 10 C/min).
-
SEM micrographs of V2O5 thin film morphology dependent on substrate types
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin film morphology dependent on substrate types. The as-prepared thin films were deposited on alumina, zirconium, zirconium oxide and metallic vanadium substrate, then was annealing under an oxidizing atmosphere at 600C for 10h. The results show that the morphology of...
-
SEM micrographs of morphology evolution of V2O5 thin films on quartz glass
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on a quartz glass substrate. The as-prepared thin films were annealing under an oxidizing atmosphere in the temperature range 200-600C. The results show that the morphology of the films dependent on the annealing temperature.
-
SEM images of symmetrical cell interface with SrTi0.65Fe0.35O3-d electrode and CGO-20 substrate in function of sintering temperature
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with SrTi0.65Fe0.35O3-d electrode and CGO-20 substrate in function of sintering temperature (800 °C, 900°C and 1000 °C) . Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage...
-
SEM images of symmetrical cell interface with SrTi0.50Fe0.50O3-d electrode and CGO-20 substrate in function of sintering temperature
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with SrTi0.50Fe0.50O3-d electrode and CGO-20 substrate in function of sintering temperature (800 °C, 900°C and 1000 °C) . Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage...
-
SEM images of symmetrical cell interface with SrTi0.30Fe0.70O3-d electrode and CGO-20 substrate in function of sintering temperature
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with SrTi0.30Fe0.70O3-d electrode and CGO-20 substrate in function of sintering temperature (800 °C, 900°C and 1000 °C) . Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage...
-
Sounding rocket temperature and heat transfer data
Open Research DataThis dataset contains temperature and heat transfer data measured during REXUS 25 sounding rocket HEDGEHOG Experiment launched from Esrange Space Centre, Kiruna, Sweden. For experiment details, please see:
-
SEM image and EDS map of SrTi0.30Fe0.70O3-d powder aglomerate
Open Research DataThis dataset contains image of the SrTi0.30Fe0.70O3-d powder aglomerate with EDS map analysis results. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage of 10 kV in a high vacuum mode. The chemical compositions of the investigated powder were determined...
-
SEM image and EDS map of SrTi0.50Fe0.50O3-d powder aglomerate
Open Research DataThis dataset contains image of the SrTi0.50Fe0.50O3-d powder aglomerate with EDS map analysis results. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage of 10 kV in a high vacuum mode. The chemical compositions of the investigated powder were determined...
-
SEM image and EDS map of SrTi0.65Fe0.35O3-d powder aglomerate
Open Research DataThis dataset contains image of the SrTi0.65Fe0.35O3-d powder aglomerate with EDS map analysis results. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage of 10 kV in a high vacuum mode. The chemical compositions of the investigated powder were determined...