Preparation to ball on disk test Initial contact stress evaluation
Open Research DataEvaluation of initial contact stress in tests on wear of Al6061 alloy in ball on disk tribological testing. Research on the reinforcing effect of aluminium alloy injection reinforcement with TiN and WC powders in laser remelted surface layer.
-
Reinforced aluminium reference measurement R63 – earlier tests
Open Research DataPreliminary testing of aluminium alloys against 100Cr6 steel ball. Preparation to tests on wear of Al6061 alloy in ball on disk experiment. Research on the reinforcing effect of aluminium alloy injection reinforcement with TiN and WC powders in laser remelted surface layer.
-
Reinforced aluminium reference measurement Result1 – earlier tests
Open Research DataPreliminary testing of aluminium alloys against 100Cr6 steel ball. Preparation to tests on wear of Al6061 alloy in ball on disk experiment. Research on the reinforcing effect of aluminium alloy injection reinforcement with TiN and WC powders in laser remelted surface layer.
-
Ball on disk test AL(rf.)-Al2O3-r25
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 25 mm. Disk material: Al6061 not treated (reference).
-
Ball on disk test AL(rf.)-Al2O3-r15
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 15 mm. Disk material: Al6061 not treated (reference).
-
Ball on disk test AT4_11-Al2O3-r25
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 25 mm. Disk material: Al6061 TiN powder injected (AT4_11).
-
Ball on disk test AT3_21-Al2O3-r25
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 25 mm. Disk material: Al6061 TiN powder injected (AT3_21).
-
Ball on disk test AW4_1-Al2O3-r15
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 15 mm. Disk material: Al6061 WC powder injected (AW4_1).
-
Ball on disk test AT4_4-Al2O3-r15
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 15 mm. Disk material: Al6061 TiN powder injected (AT4_4).
-
Ball on disk test AW4_11-Al2O3-r25
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 25 mm. Disk material: Al6061 WC powder injected (AW4_11).
-
Ball on disk test AT4_1-Al2O3-r15
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 15 mm. Disk material: Al6061 TiN powder injected (AT4_1).
-
Ball on disk test AT4_41-Al2O3-r25
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 25 mm. Disk material: Al6061 TiN powder injected (AT4_41).
-
Ball on disk test AT3_2-Al2O3-r15
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 15 mm. Disk material: Al6061 TiN powder injected (AT3_2).
-
Ball on disk test AW4_4-Al2O3-r15
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 15 mm. Disk material: Al6061 WC powder injected (AW4_4).
-
Ball on disk test AW4_41-Al2O3-r25
Open Research DataHard particle reinforced Al6061 alloy testing. Laser remelting and kinetic injection of particulate material. Ball on disc tribological test. Ball material: Al2O3. Ball diameter: 5 mm. Sliding path radius: 25 mm. Disk material: Al6061 WC powder injected (AW4_41).
-
Microscopic examination of CuNiFeR pipeline
Open Research DataCopper and nickel alloys called cunifers (Cu, Ni, Fe and R – rest of alloy elements) have found wide application in the production of ship pipeline components in contact with sea water, such as, for example, the main engine cooling system. These alloys are characterized by a very high corrosion resistance, which is ensured by appropriately carried out...
-
Macroscopic examination of CuNiFeR pipeline
Open Research DataCopper and nickel alloys called cunifers (Cu, Ni, Fe and R – rest of alloy elements) have found wide application in the production of ship pipeline components in contact with sea water, such as, for example, the main engine cooling system. These alloys are characterized by a very high corrosion resistance, which is ensured by appropriately carried out...
-
Tensile test of part of CuNiFeR pipeline
Open Research DataCopper and nickel alloys called cunifers (Cu, Ni, Fe and R – rest of alloy elements) have found wide application in the production of ship pipeline components in contact with sea water, such as, for example, the main engine cooling system. These alloys are characterized by a very high corrosion resistance, which is ensured by appropriately carried out...
-
Identification of intermetallic phases in the structure of austenitic steel with use of Scanning Kelvin Probe Microscopy
Open Research DataDelta ferrite is formed in austenitic steels during the solidification of the alloy and its welds. It can also occur as a stable phase in any temperature range in high-alloy austenitic-ferritic steels. Depending on the amount, it can change into gamma and sigma phases and into ferrite with variable chromium content. The main role of delta ferrite in...
-
SEM micrographs of aluminium corrosion in alkaline media with various bee products as corrosion inhibitors
Open Research DataThis dataset contains various scanning electron microscopy (SEM) micrographs of AA5754 aluminum alloy samples exposed to the corrosive alkaline environment without and with the addition of various bee products to act as green corrosion inhibitors. The products are bee pollen, honey, and putty. They were investigated in bicarbonate buffer (pH =10 or...