Brunauer-Emmett-Teller (BET) surface analysis of titanium dioxide (TiO2) and silicon dioxide (SiO2) used for coating of expanded polystyrene spheres (EPS) - Open Research Data - MOST Wiedzy

Wyszukiwarka

Brunauer-Emmett-Teller (BET) surface analysis of titanium dioxide (TiO2) and silicon dioxide (SiO2) used for coating of expanded polystyrene spheres (EPS)

Opis

Data refer to the results of BET surface area of TiO2 and SiO2 powders used for coating of expanded polystyrene spheres. The detailed measurement and equipment data was described in readme BET.txt file.
TiO2 was treated firstly in autoclave at 150 C degrees for 1h, then was further heat treated in Ar at 400 C degrees. As a raw material TiO2 was used, which was a semiproduct from the industrial production of titania white by sulphur method. The raw material was mostly amorphous and contained some nuclei of rutile and sulphur species. SiO2 was obtained via modified Strober method.

Plik z danymi badawczymi

BET.zip
32.7 kB, S3 ETag db97efc2a4ce26c087c38635a0669243-1, pobrań: 62
Hash pliku liczony jest ze wzoru
hexmd5(md5(part1)+md5(part2)+...)-{parts_count} gdzie pojedyncza część pliku jest wielkości 512 MB

Przykładowy skrypt do wyliczenia:
https://github.com/antespi/s3md5
pobierz plik BET.zip

Informacje szczegółowe o pliku

Licencja:
Creative Commons: by 4.0 otwiera się w nowej karcie
CC BY
Uznanie autorstwa

Informacje szczegółowe

Rok publikacji:
2024
Powiązana lokacja:
Szczecin, województwo zachodniopomorskie, Polska (53° 25′ 29″ N, 14° 32′ 8″ E)
Data zatwierdzenia:
2024-02-12
Data wytworzenia:
2023
Język danych badawczych:
angielski
Dyscypliny:
  • inżynieria materiałowa (Dziedzina nauk inżynieryjno-technicznych)
DOI:
Identyfikator DOI 10.34808/7k25-jw97 otwiera się w nowej karcie
Finansowanie:
Weryfikacja:
Zachodniopomorski Uniwersytet Technologiczny w Szczecinie

Słowa kluczowe

Powiązane zasoby

Cytuj jako

eksportuj:

Trwa wczytywanie...

wyświetlono 159 razy