Opis

The DataSet contains the nanoindentation curves (indentation force Fn vs penetrationPd) for a single V2O5 nanocrystal supported on a substrate. The measurements were performed in control of the maximum load of  Berkovich indenter force from 2 to 50 mN. 

Nanoindentation curves were collected on a Nanoidenter TTX-NHT2 CSM. The details about measurements are included in each .text file.

Plik z danymi badawczymi

max load.zip
212.6 kB, S3 ETag 81af174058f4e89dbf7dd76234bd2415-1, pobrań: 54
Hash pliku liczony jest ze wzoru
hexmd5(md5(part1)+md5(part2)+...)-{parts_count} gdzie pojedyncza część pliku jest wielkości 512 MB

Przykładowy skrypt do wyliczenia:
https://github.com/antespi/s3md5
pobierz plik max load.zip

Informacje szczegółowe o pliku

Licencja:
Creative Commons: by 4.0 otwiera się w nowej karcie
CC BY
Uznanie autorstwa
Dane surowe:
Dane zawarte w datasecie nie zostały w żaden sposób przetworzone.

Informacje szczegółowe

Rok publikacji:
2021
Data zatwierdzenia:
2021-06-21
Język danych badawczych:
angielski
Dyscypliny:
  • inżynieria materiałowa (Dziedzina nauk inżynieryjno-technicznych)
DOI:
Identyfikator DOI 10.34808/jprz-7a38 otwiera się w nowej karcie
Seria:
Weryfikacja:
Politechnika Gdańska

Słowa kluczowe

Powiązane zasoby

Cytuj jako

wyświetlono 111 razy