Optical microsc. images of wear marks on ball (JPG). Reciprocating siding friction tests. Ball-on-flat contact. Sintered alumina ceramics (98%). No lubrication (DRY). Specim. set K03
Opis
Optical microscope images of wear zone on the 5mm diam. ceramic ball used in tests as the fixed specimen.
Friction and wear tests in ball-on-flat contact. Both specimens made of sintered alumina ceramics (98%) - self-mated contact.
Linear reciprocating motion.
Lubrication: DRY. Sliding velocity (peak): 0.1 m/s. Load (normal force): 5N. Test rig: TPZ-1 Tribometer.
Running time: progressive increments of 10, 15, 30, 60, 180 and 300s. Wear mark examination at each intermission between test segments.
Specimen set K03
Plik z danymi badawczymi
K03.rar
4.1 MB,
S3 ETag
3bca3dbc6dcfcf9b7740767f7da56744-1,
pobrań: 43
Hash pliku liczony jest ze wzoru
Przykładowy skrypt do wyliczenia:
https://github.com/antespi/s3md5
hexmd5(md5(part1)+md5(part2)+...)-{parts_count}
gdzie pojedyncza część pliku jest wielkości 512 MBPrzykładowy skrypt do wyliczenia:
https://github.com/antespi/s3md5
Informacje szczegółowe o pliku
- Licencja:
-
otwiera się w nowej karcieCC BY-NCUżycie niekomercyjne
- Dane surowe:
- Dane zawarte w datasecie nie zostały w żaden sposób przetworzone.
Informacje szczegółowe
- Rok publikacji:
- 2021
- Data zatwierdzenia:
- 2021-05-30
- Język danych badawczych:
- angielski
- Dyscypliny:
-
- inżynieria mechaniczna (Dziedzina nauk inżynieryjno-technicznych)
- inżynieria materiałowa (Dziedzina nauk inżynieryjno-technicznych)
- DOI:
- Identyfikator DOI 10.34808/7fgv-g450 otwiera się w nowej karcie
- Seria:
- Weryfikacja:
- Politechnika Gdańska
Słowa kluczowe
Cytuj jako
Autorzy
wyświetlono 84 razy