Filtry
wszystkich: 703
wybranych: 86
Wyniki wyszukiwania dla: PATTERN
-
The XRD pattern of CeO2/10wt.%Ni with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Ni. The samples of nanoCeO2 were impregnated with BCD-assisted precursor nitrate solution (betacyclodextrin). The dataset includes 5-90 2 theta degree measurement. Nonreduced. Sintered at 400oC for 4h.
-
The XRD pattern of CeO2/10wt.%Co prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Co. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement.
-
The XRD pattern of CeO2/10wt.%Ni prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Ni. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4h in air.
-
The XRD pattern of CeO2/10wt.%Mn prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Mn. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Fe prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Fe. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Cu prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Cu. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Cu prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Cu. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Fe prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Fe. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Mn prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Mn. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Co prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Co. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Ni prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Ni. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
XRD pattern of Mo2Ga2C, Mo2CTx/Mo2GaC and Ni-Mo2CTx/Mo2Ga2C materials
Dane BadawczeIn the dataset are included raw data for the preparation of XRD pattern of Mo2Ga2C, Mo2CTx/Mo2GaC and Ni-Mo2CTx/Mo2Ga2C materials.
-
Powder x-ray diffraction pattern of polycrystalline synthetic leningradite, PbCu3V2O8Cl2
Dane BadawczePolycrystalline sample of Cu2+ (S=1/2) antiferromagnetic PbCu3V2O8Cl2 (synthetic analogue of the mineral leningradite) was prepared by solid state reaction of PbCl2, CuO, and V2O5.
-
Radiation pattern measurements of geometrically small antennas performed in non-anechoic environments
Dane BadawczeThe dataset contains unprocessed measurements of radiation pattern characteristics performed in non-anechoic regime for three geometrically small antenna structures: a spline-parameterized Vivaldi structure, a compact spline-based monopole, and a quasi-Yagi geometry with enhanced bandwidth. The responses have been obtained over broad frequency ranges...
-
Powder x-ray diffraction pattern of polycrystalline Cu(IO3)2*xH2O
Dane BadawczeHydrated copper(II) iodate sample was prepared in water solution by reacting copper(II) sulfate and potassium iodate, following the method described by Peterson (J. Chem. Educ. 1957, 34, 12, 612). The sample was subsequently dried at various temperatures in order to produce an anhydrous Cu(IO3)2:
-
The XRD diffraction pattern of interdiffusion test in the CLO-NiO-YSZ system (30wt.%YSZ)
Dane BadawczeThe dataset includes the XRD pure diffraction pattern of the interdiffusion system consisting of CLO (Ce0.8La0.2O2), NiO and 8YSZ (8mol.% Y2O3 stabilized ZrO2). The mixture contains equal amounts of CLO and NiO as well as 30wt.% 8YSZ. Samples were sintered at 1400 oC. The reaction between CLO and YSZ is visible.
-
The XRD diffraction pattern of interdiffusion test in the CLO-NiO-YSZ system (10wt.%YSZ)
Dane BadawczeThe dataset includes the XRD pure diffraction pattern of the interdiffusion system consisting of CLO (Ce0.8La0.2O2), NiO and 8YSZ (8mol.% Y2O3 stabilized ZrO2). The mixture contains equal amounts of CLO and NiO as well as 10wt.% 8YSZ. Samples were sintered at 1400 oC. The reaction between CLO and YSZ is visible.
-
The XRD diffraction pattern of interdiffusion test in the CLO-NiO-YSZ system (20wt.%YSZ)
Dane BadawczeThe dataset includes the XRD pure diffraction pattern of the interdiffusion system consisting of CLO (Ce0.8La0.2O2), NiO and 8YSZ (8mol.% Y2O3 stabilized ZrO2). The mixture contains equal amounts of CLO and NiO as well as 20wt.% 8YSZ. Samples were sintered at 1400 oC. The reaction between CLO and YSZ is visible.
-
XRD patterns of nickel-modified V2CTx
Dane BadawczeThe set includes data for XRD pattern preparation of nickel-modified V2CTx samples.
-
XRD patterns of MXenes catalysts
Dane BadawczeData contain results from XRD measurements of the Ti3C2Tx MXenes produced via acidic etching aluminum from MAX Phase (Ti3C2-Al-Ti3C2-Al-Ti3C2) using different etching agents, HF/HCl and HF/H2SO4 with different weight ratios (1:3, 1:4, and 1:5). The samples were labeled as MXene HF/HCl X:Y and MXene HF/H2SO4 X:Y, where X:Y means the acids weight ratios....