Wyniki wyszukiwania dla: TRANSITION METALS
-
The reductivity of the transition metals - calculations
Dane BadawczeThe dataset includes the reduction enthalpy and Gibbs energy simulated for Co, Cu, Fe, La, Mo, Ni, Sr, Ti, and W from oxide form into metallic form in hydrogen. Simulations were performed using HSC Chemistry software.
-
The 2p XPS spectra of transition metals in Ce0.9M0.1O2
Dane BadawczeThe dataset consists of 2p XPS spectra of transition metals in Ce0.9M0.1O2 where (M=Mn, Fe, Co, Ni, Cu). X-ray Photoelectron Spectroscopy analysis (XPS) was performed using X-ray photoelectron spectrometer Omnicron NanoTechnology with 128-channel collector. XPS measurements were undertaken in ultra-high vacuum conditions, below 1.1x10-8 mbar. Photoelectrons...
-
X-Ray photoemission spectroscopy measurements of the Nb-V-Sr-O ceramics
Dane BadawczeNiobium doped strontium vanadate based perovskite SrV1-xNbxO3-δ materials were prepared via conventional solid state reaction (SSR) method. For comparison, different samples with a various amount of niobium dopant in the structure were synthesized; x = 0; 0,2; 0,5; 0,8 and 1. Samples were sintered by two-steps: first under a pure hydrogen (purity >99.999%)...
-
The chemical and mechanical pressure influence on chromium luminescence
Dane BadawczeIn this study, we aim to compare the changes in the luminescence properties of Ga2O3:Cr3+ modified by Al or Sc ion substitution (chemical pressure) and hydrostatic pressure. We find the same behavior for Ga2–xAlxO3:Cr3+ and different behavior for Ga2–xScxO3:Cr3+ in terms of the optical properties under chemical and mechanical pressure. We consider Al...
-
The electrical properties mesurements of DIR-SOFC with CeO2-s functional layer
Dane BadawczeThe dataset includes the electrical properties mesurements of SOFC with CeO2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
The electrical properties mesurements of DIR-SOFC with Ce0.8Cu0.2O2-s functional layer
Dane BadawczeThe dataset includes the electrical properties mesurements of SOFC with Ce0.8Cu0.1O2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
The electrical properties mesurements of DIR-SOFC with Ce0.8Fe0.2O2-s functional layer
Dane BadawczeThe dataset includes the electrical properties mesurements of SOFC with Ce0.8Fe0.1O2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
The electrical properties mesurements of DIR-SOFC with Ce0.8Co0.2O2-s functional layer
Dane BadawczeThe dataset includes the electrical properties mesurements of SOFC with Ce0.8Co0.1O2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
The electrical properties mesurements of DIR-SOFC with Ce0.8Mn0.2O2-s functional layer
Dane BadawczeThe dataset includes the electrical properties mesurements of SOFC with Ce0.8Mn0.1O2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
The electrical properties mesurements of DIR-SOFC with Ce0.8Ni0.2O2-s functional layer
Dane BadawczeThe dataset includes the electrical properties mesurements of SOFC with Ce0.8Ni0.1O2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
The XRD pattern of CeO2/10wt.%Cu prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Cu. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Fe prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Fe. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Mn prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Mn. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Mn prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Mn. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Fe prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Fe. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Co prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Co. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Ni prepared without BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Ni. The samples of nanoCeO2 were impregnated without BCD-assisted precursor solution (betacyclodextrin) - pure nitarte solution 1M. The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Ni with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Ni. The samples of nanoCeO2 were impregnated with BCD-assisted precursor nitrate solution (betacyclodextrin). The dataset includes 5-90 2 theta degree measurement. Nonreduced. Sintered at 400oC for 4h.
-
The XRD pattern of CeO2/10wt.%Cu prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Cu. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4 h in air.
-
The XRD pattern of CeO2/10wt.%Ni prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Ni. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement. Nonreduced. Sintered at 400oC for 4h in air.
-
The XRD pattern of CeO2/10wt.%Co prepared with BCD
Dane BadawczeThe dataset includes the XRD pattern of CeO2/10wt.%Co. The samples of nanoCeO2 were impregnated with BCD-assisted precursor solution (betacyclodextrin). The dataset includes the 5-90 2theta degree measurement.