Didn't find any results in this catalog!
But we have some results in other catalogs.Search results for: titanium alloy ti13nb13zr
-
Preparation of nano-tubular oxide layers on titanium alloy Ti13Nb13Zr
PublicationThe article presents results of oxidation tests and corrosion investigations of titanium alloy Ti13Nb13Zr preformed at different conditions. The oxide layers have been formed using electrochemical method in 2M H3PO4 + 0,3% HF solution for 30 min. and 1h at 20V constant voltage. The corrosion tests heve been made with poteniodynamic method in Ringer's solution at pH ranged 3 and 7. It has been shown that the nano-oxide films, which...
-
Nanotubular oxide layers and hydroxyapatite coatings on porous titanium alloy Ti13Nb13Zr
PublicationThe surface condition of an implant has a significant impact on response occurring at the implant-biosystem border. The knowledge of physical-chemical and biological processes allows for targeted modification of biomaterials to induce a specified response of a tissue. The present research was aimed at development of technology composing of obtaining the nanotube oxide layers on a porous titanium alloy Ti13Nb13Zr, followed by the...
-
Mechanical Properties and Wear Susceptibility Determined by Nanoindentation Technique of Ti13Nb13Zr Titanium Alloy after “Direct Laser Writing”
PublicationLaser treatment has often been applied to rebuild the surface layer of titanium and its alloys destined for long-term implants. Such treatment has always been associated with forming melted and re-solidified thin surface layers. The process parameters of such laser treatment can be different, including the patterning of a surface by so-called direct writing. In this research, pulse laser treatment was performed on the Ti13Nb13Zr...
-
Elctrochemical oxidation and corrosion resistance of the Ti13Nb13Zr alloy
PublicationThis paper presents the results of oxidation and corrosion tests carried out on titanium alloy Ti13Nb13Zr. The oxide film was prepared by electrochemical environment 2M H3PO4 for 30 min and 1 h, at a constant voltage 40V. The tests of corrosion resistance were performed by potentiostatic method in Ringer's solution at different pH values: 7, 5 and 3. The change in an appearance of surface and the increase in corrosion resistance...
-
Effect of hybrid modification by ceramic layer formation in MAO process and laser remelting on the structure of titanium bio-alloy Ti13Nb13Zr
PublicationTo improve the biological properties of titanium alloy Ti13Nb13Zr, hybrid modifications involving micro-arc oxidation (MAO) and Nd: YAG laser remelting were carried out in two combinations. The first consisted of laser modification before the production of the ceramic layer by the micro-arc oxidation process, and the second combination involved Nd: YAG laser modification after the MAO process. The creation of developed surface...
-
Properties of Composite Oxide Layers on The Ti13Nb13Zr Alloy
PublicationThe development of composite oxide layers on the Ti13Nb13Zr alloy, their structure and properties have been demonstrated. Two subsequent methods were applied to prepare the composite layers. During the first stage gas oxidation produced a solid oxide layer, and subsequently oxide nanotubes were produced by using an electrochemical method. Scanning electron microscopy (SEM), chemical analysis, energy dispersive X-ray spectroscopy...
-
Hydroxyapatite deposition on the laser modified Ti13Nb13Zr alloy
PublicationThe Ti13Nb13Zr alloy was subjected to laser modification with the Nd:YAG laser provided that such treatment would increase the surface roughness followed improved adhesion of hydroxyapatite (HAp) coatings The hydroxyapatite was deposited by electrophoretic method in suspension of 0.5 g HA powder and 100 ml ethyl alcohol. The deposition was carried out for 10 min at 10 V voltage followed by drying at room temperature for 24 h and...
-
Surface treatment of porous Ti13Nb13Zr alloy for biomedical applications
PublicationPrzeprowadzono badania materiału porowatego, przeznaczonego na implanty ortopedyczne, wytworzonego metodą metalurgii proszków ze stopu Ti13Nb13Zr. Proszki z badanego stopu uzyskano metodą rozpylania plazmowego. Otrzymano próbki o otwartej porowatej strukturze, stopniu porowatości do 68% i średniej wielkości porów w przedziale 30-150 mikrometrów. Obróbka próbek porowatych - utlenianie termiczne, chemiczne i/lub elektrochemiczne...
-
Environmental degradation of titanium alloy in artificial saliva
PublicationThe titanium and its alloys are potentially prone to hydrogen embrittlement, including those proposed for dental implants. The research has been aimed to assess a susceptibility to environment-enhanced degradation of the Ti-13Zr-13Nb alloy in artificial saliva with or without hydrofluoric acid, subject or not to cathodic polarisation. The results have shown that even if artificial saliva is safe environment, both cathodic polarization...
-
Mechanical and Corrosion Properties of Laser Surface-Treated Ti13Nb13Zr Alloy with MWCNTs Coatings
Publication: Titanium and its alloys is the main group of materials used in prosthetics and implantology. Despite their popularity and many advantages associated with their biocompatibility, these materials have a few significant disadvantages. These include low biologic activity—which reduces the growth of fibrous tissue and allows loosening of the prosthesis—the possibility of metallosis and related inflammation or other allergic reactions,...