Filters
total: 32
filtered: 24
Chosen catalog filters
Search results for: BERYLLIUM-TELLURIUM-IRON GLASSES
-
Linear and nonlinear impedance of iron containing silicate glasses
Open Research DataThe linear and nonlinear impedance ofglasses doped with iron oxide were measured. Glass samples (50 SiO2-50-xPbO-xFe2O3 in mol%) were prepared by the conventional melt quenching technique. The substrates were powdered in a mortar and melted in Al2O3 crucibles. The melting was conducted in air at 1623K. The melts were poured out on plate heated up to...
-
The structure of lead-silicate glasses and nanocomposites doped with iron oxide
Open Research DataThe structure of iron-doped glasses and glass-ceramics were studied. Samples has the composition of 50SiO2–(50−x)PbO–xFe2O3, where x=15, 20 and 25 (in mol%). All samples were prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass plate preheated to 573...
-
The morphology of lead-silicate glasses and nanocomposites doped with iron oxide
Open Research DataThe topography of iron-doped glasses and glass-ceramics were studied. Samples has the composition of 50SiO2–(50−x)PbO–xFe2O3, where x=15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass plate preheated to 573...
-
The morphology of lead-silicate glasses containing nanocrystallites of iron oxides
Open Research DataThe topography of iron-doped glasses and glass-ceramics were studied. Samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass...
-
The structure of lead-silicate glasses containing nanocrystallites of iron oxides
Open Research DataThe structure of iron-doped glasses and glass-ceramics were studied. Samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All samples were prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass...
-
Linear and nonlinear impedance of alkali and iron doped silicate-lead glasses
Open Research DataLinear and nonlinear impedance was studied for lead-silicate glass samples doped with iron ions and alkaline oxides. The compositions of glasses were as follows: (in %mol) 50% SiO2, 25% PbO, 15% Fe2O3 and 15% one of alkaline oxides: Na2O, K2O, Li2O. All samples were prepared by the conventional melt quenching technique. The substrates were powdered...
-
The morphology of lead-borate glasses and nanocomposites doped with iron oxide
Open Research DataThe topography of iron-doped borate glasses and glass-ceramics were studied. Samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 < x < 37 in mol%) were prepared by the conventional meltquenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate...
-
The structure of lead-borate glasses containing nanocrystallites of iron oxides
Open Research DataThe structure of iron-doped glasses and glass-ceramics were studied. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate and...
-
Topography and microstructure of phosphate-iron glasses containing niobium and titanium
Open Research DataThe topography and microstructure of phosphate-iron glasses containing niobium and titanium were investigated by the means of X-ray diffraction (XRD), scanning electron microscopy (SEM). Glass samples of the composition of 35P2O5-30Fe2O3-(35-x)Nb2O5-xTiO2 where x= 0; 7.5 and 15 (in %mol) were prepared by the conventional melt quenching technique. Appropriate...
-
Magnetic properties of of lead-silicate glasses and nanocomposites doped with iron oxide
Open Research DataMagnetic properties of iron-doped glasses and glass-ceramics were studied. Two different sets of glass samples were prepared. The first group of samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO– xFe2O3, where x = 15 and 20 (in mol%). Composition of the second group was 50SiO2–(50−x)PbO–xFe2O3, where x=15, 20 and 25 (in mol%). All sampleswere...
-
Electrical properties of silicate-lead glasses containing nanostructures of iron oxides.
Open Research DataElectrical properties of silicate-lead glasses doped with different content of iron oxide was studied. The set of glass samples were prepared with the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in...
-
Electrical properties of nanostructures in lead-silicate glasses and nanocomposites doped with iron oxide
Open Research DataElectrical properties of iron oxide nanostructures observed in silicate glasses and glass-ceramics were studied. Two different sets of glass samples were prepared. The first group of samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO– xFe2O3, where x = 15, 20 and 25 (in mol%). Composition of the second group was 50SiO2–(50−x)PbO–xFe2O3, where...
-
Electrical properties of lead-borate glasses and glass-ceramics containing iron ions
Open Research DataElectrical properties were studied for borate-lead glasses and glass-ceramics doped with iron ions. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated...
-
Topography of iron-phosphate glasses doped with niobium and titanium tested by confocal microscope
Open Research DataThe topography of phosphate-iron glasses containing niobium and titanium were investigated with the use of confocal miscroscope. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5, 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 and 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents...
-
Detection of the Ag nanoparticles in Te-Bi-Ba-Oa glass
Open Research DataThe influence of the manufacturing parameters of tellurium-bismuth-barium glasses on the presence of silver nanoparticles was investigated. Glasses were annealed at 330, 335, 340, 345 and 350 degrees Celsius for 24 and 48 hours. Presence of the Ag nanoparticles was measured by XPS method. The growth of nanoparticles was observed along with the extension...
-
XPS measurements of the Fe-Bi based glass
Open Research DataFe-Si-O and Fe-Si-Pb-O glass was measured by XPS method. The influence of Pb dopand on the glass structure, including the valence of iron, was investigated. The influence of the annealing temperature on the behavior of iron in glass was also investigated. Studies have confirmed the mixed valence of iron in glasses and a high proportion of metallic Fe.
-
Linear impedance of 35P2O5-30Fe2O3-20Nb2O5-15TiO2
Open Research DataThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Open Research DataThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and...
-
Linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Open Research DataThe electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2 (≥99.9%, anatase...
-
High temperature linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Open Research DataThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...
-
High temperature linear impedance of 35P2O5-30Fe2O3-25Nb2O5-15TiO2
Open Research DataThe high temperature electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%,...
-
High temperature linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Open Research DataThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-35Nb2O5 glass
Open Research DataThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH) and Nb2O5 (≥99.9%, PLUKA AG) were...
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 glass
Open Research DataThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...