Search results for: ELECTROCHEMICAL IMPEDANCE
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 partially crystallized glass at 613 K measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 partially crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for fully crystallized 45Bi2VO5.5-55SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties as a function of A.C. voltage for fully crystallized 45Bi2VO5.5-55SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 30Bi2VO5.5-70SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 30Bi2VO5.5-70SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized was measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized was measured by impedance spectroscopy method.
-
Silicon microcantilever with impedance sensor
Open Research DataThe issue of microelectromechanical systems (MEMS) [1] has been enjoying popularity and interest since the 90s of the 20th century. Microcells are one of the simplest devices of this type, but they can be widely used in sensors. There are reports on the possibility of using this type of sensors in the context of such important issues as diagnostics...
-
Electrical properties of silicate-lead glasses containing nanostructures of iron oxides.
Open Research DataElectrical properties of silicate-lead glasses doped with different content of iron oxide was studied. The set of glass samples were prepared with the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in...
-
Electrical properties of lead-borate glasses and glass-ceramics containing iron ions
Open Research DataElectrical properties were studied for borate-lead glasses and glass-ceramics doped with iron ions. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated...
-
Austenitic stainless steel sensitization
Open Research DataHigh-alloy steels, thanks to their composition and content of appropriate alloying additives, are characterized by increased resistance to many corrosive environments. However, this is due to the increased sensitivity of the described construction materials to specific environmental conditions during their use. An example may be the increased susceptibility...
-
Linear impedance of 35P2O5-30Fe2O3-20Nb2O5-15TiO2
Open Research DataThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Open Research DataThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and...
-
Linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Open Research DataThe electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2 (≥99.9%, anatase...
-
High temperature linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Open Research DataThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...
-
High temperature linear impedance of 35P2O5-30Fe2O3-25Nb2O5-15TiO2
Open Research DataThe high temperature electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%,...
-
High temperature linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Open Research DataThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Ni/cerium Molybdenum Oxide Hydrate Microflakes Composite Coatings Electrodeposited from Choline Chloride: Ethylene Glycol Deep Eutectic Solvent
PublicationCerium molybdenum oxide hydrate microflakes are codeposited with nickel from a deep eutectic solvent-based bath. During seven days of exposure in 0.05 M NaCl solution, the corrosion resistance of composite coating (Ni/CeMoOxide) is slightly reduced, due to the existence of some microcracks caused by large microflakes. Multielemental analysis of the solution, in which coatings are exposed and the qualitative changes in the surface...